Polymer Property : Tensile Modulus = 68.9 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.475 GPa

@Temperature 23.0 °C
68.9 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® FN714 NC010A Nylon 66
Zytel® FN714 NC010A is an impact modified, very flexible, plasticizer free polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers
Tensile Modulus 0.475 GPa
68.9 ksi
1 mm/min
Arkema Group Rilsan® AESN P302 TL Nylon 12, Flexible Tubing Grade (Dry)
(Former designation: RILSAN MA 4403)Designation ISO 1874-PA12-HI,EHL,22-003Flexible grade for tubes extrusion. Available color: black. Light and thermal stabilized.Flexibility. High burst pressure a..