Polymer Property : Dielectric Strength = 1030 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 40.7 kV/mm
1030 kV/in
Arkema Group Rilsan® AESN P302 TL Nylon 12, Flexible Tubing Grade (Dry)
(Former designation: RILSAN MA 4403)Designation ISO 1874-PA12-HI,EHL,22-003Flexible grade for tubes extrusion. Available color: black. Light and thermal stabilized.Flexibility. High burst pressure a..