AdvanSource Biomaterials ChronoThane™ P Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer AdvanSource Biomaterials (formerly CardioTech International)
Trade Name ChronoThane™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AdvanSource Biomaterials ChronoThane™ P Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AdvanSource Biomaterials Corporation manufactures and markets aromatic-based ChronoThane™ P. Some characteristics that have made it attractive to medical device manufacturers include low coefficient of friction, low extractables, dimensional stability, gamma sterilizable, chemical inertness, and biodurability. In addition, they are coupled with easy thermoplastic processability. Hardnesses from 80 Shore A to 75 Shore D are available; property data below is typical for 80A.Information provided by AdvanSource Biomaterials Corporation.
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength, Ultimate 35.2 MPa
5100 psi
ASTM D412
Elongation at Break 550 %
550 %
ASTM D412
100% Modulus 0.00586 GPa
0.850 ksi
300% Modulus 0.0121 GPa
1.75 ksi
Flexural Modulus 0.103 GPa
15.0 ksi
ASTM D790
Tear Strength 73.6 kN/m
420 pli
Die C; ASTM D624
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
Processing Properties Metric English Comments
Zone 1 193 °C
380 °F
Zone 2 193 °C
380 °F
Zone 3 193 °C
380 °F
Die Temperature 204 °C
400 °F
Melt Temperature 210 °C
410 °F
Drying Temperature 73.9 - 79.4 °C
165 - 175 °F
Dry Time 3 - 4 hour
3 - 4 hour
Moisture Content <= 0.10 %
<= 0.10 %
Dew Point -40.0 °C
-40.0 °F