Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0121 GPa | 1.75 ksi | aged 70 hours at 300ºF |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0121 GPa | 1.75 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0121 GPa | 1.75 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Monoplex DOS Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0121 GPa | 1.75 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Plasticizer SC MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0121 GPa @Temperature 145 °C, Time 2990 sec |
1.75 ksi @Temperature 293 °F, Time 0.830 hour |
cured; ASTM D412 |
LG Chemical NBR 6240 High Acrylonitrile Polymer Description: NBR 6240 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6240 is a non staining, medium low mooney.. |
|||
300% Modulus | 0.0121 GPa | 1.75 ksi | ASTM D412 |
Lubrizol Pellethane® 2363-80A Thermoplastic Polyurethane Elastomer Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
300% Modulus | 0.0121 GPa | 1.75 ksi | ASTM D412 |
UBE UBEPOL VCR406 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
300% Modulus | 0.0121 GPa | 1.75 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Plasticizer SC MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0121 GPa | 1.75 ksi | aged 70 hours at 300ºF |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0121 GPa | 1.75 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0121 GPa | 1.75 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Monoplex DOS Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0121 GPa | 1.75 ksi | ASTM D412 |
Lubrizol Estane® 2103-85AE Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in.. |
|||
300% Modulus | 0.0121 GPa | 1.75 ksi | |
AdvanSource Biomaterials ChronoThane™ P Thermoplastic Polyurethane Elastomer AdvanSource Biomaterials Corporation manufactures and markets aromatic-based ChronoThane™ P. Some characteristics that have made it attractive to medical device manufacturers include low coefficien.. |