Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 204 °C | 400 °F | Extrusion |
ExxonMobil Santoprene® 241-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Die Temperature | 204 °C | 400 °F | Extrusion |
ExxonMobil Vyram™ 9101-65 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Die Temperature | 204 °C | 400 °F | Extrusion |
ExxonMobil Vyram™ 9101-75 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Die Temperature | 204 - 218 °C | 400 - 425 °F | |
LyondellBasell Petrothene® GA837091 Medium Density Polyethylene
(Unverified Data**) ApplicationsPETROTHENE GA 837-091 is a broad molecular weight, medium density resin designed for use as a base resin in wire and cable jacketing. An antioxidant has been added to ensure thermal st.. |
|||
Die Temperature | 204 - 218 °C | 400 - 425 °F | |
LyondellBasell Petrothene® GA808091 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 808-091 is a broad molecular weight, linear low density polyethylene resin designed for use as a base resin in wire and cable jacketing. An antioxidant package is added to.. |
|||
Die Temperature | 204 - 218 °C | 400 - 425 °F | |
LyondellBasell Petrothene® HR92953 Medium Density Polyethylene ApplicationsPETROTHENE HR 92953 is a medium density polyethylene-based resin designed for use as jacketing for communications cable, including CATV and FOC. HR 92953 has a nominal carbon black cont.. |
|||
Die Temperature | 204 - 218 °C | 400 - 425 °F | |
LyondellBasell Petrothene® NA217080 Low Density Polyethylene ApplicationsPETROTHENE NA 217-080 is a natural low density polyethylene resin formulated for use as primary insulation for coaxial and control cable applications. NA 217-080 has also been designed .. |
|||
Die Temperature | 204 - 218 °C | 400 - 425 °F | |
LyondellBasell Petrothene® PR92735 Linear Low Density Polyethylene ApplicationsPETROTHENE PR 92735 is a high molecular weight, linear low density-based compound designed for cable jacketing. PR 92735 contains a nominal carbon black content of 2.6% and antioxidant .. |
|||
Die Temperature | 204 °C | 400 °F | |
Multibase Multi-Flex® A 5001 LC TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, GoodWe.. |
|||
Die Temperature | 204 °C | 400 °F | |
Multibase Multi-Flex® A 7204 LC TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Die Temperature | 204 °C | 400 °F | |
Multibase Multi-Flex® A 7455 ER TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Die Temperature | 204 °C | 400 °F | |
Multibase Multi-Flex® D 4003 Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection MoldingExtrusion Information provided by Multibase |
|||
Die Temperature | 204 °C | 400 °F | |
DuPont Nucrel® 699 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Die Temperature | 204 °C | 400 °F | |
DuPont Nucrel® 925 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 925 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Die Temperature | 204 °C | 399 °F | Zone 2, Extrusion |
Lubrizol ESTANE® 58226 Ester Based Thermoplastic Polyurethane Features: Excellent physical properties, good chemical resistance and enhanced hydrolysis resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and.. |
|||
Die Temperature | 204 °C | 399 °F | Zone 2, Extrusion |
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an.. |
|||
Die Temperature | 204 °C | 400 °F | |
DuPont Nucrel® 599 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Die Temperature | 204 °C | 400 °F | |
DuPont Nucrel® 960 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Die Temperature | 204 °C | 400 °F | Extrusion |
ExxonMobil Santoprene® 201-80 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Die Temperature | 204 °C | 400 °F | Extrusion |
ExxonMobil Santoprene® 241-73W236 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and contains.. |
|||
Die Temperature | 204 °C | 400 °F | Extrusion |
ExxonMobil Santoprene® 241-80W236 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and contains.. |
|||
Die Temperature | 204 °C | 400 °F | Extrusion |
ExxonMobil Santoprene® 121-80 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
Die Temperature | 204 °C | 400 °F | Extrusion |
ExxonMobil Santoprene® 171-73 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Die Temperature | 204 - 221 °C | 400 - 430 °F | Average value: 214 °C Grade Count:3 |
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and.. |
|||
Die Temperature | 204 °C | 400 °F | Extrusion |
ExxonMobil Santoprene® 241-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Die Temperature | 204 °C | 400 °F | Extrusion |
ExxonMobil Vyram™ 9201-55 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Die Temperature | 204 °C | 400 °F | Extrusion |
ExxonMobil Vyram™ 9201-75 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Die Temperature | 204 °C | 400 °F | |
Multibase Multi-Flex® A 8103 E Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection MoldingExtrusions Information provided by Multibase |
|||
Die Temperature | 204 °C | 400 °F | Extrusion |
ExxonMobil Santoprene® 201-73W175 Thermoplastic Elastomer
(discontinued **) A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for thin wall .. |
|||
Die Temperature | 204 °C | 400 °F | Extrusion |
ExxonMobil Santoprene® 221-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |