Mechanical Properties Metric English Comments
300% Modulus 0.0121 GPa
1.75 ksi
aged 70 hours at 300ºF
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical)
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.0121 GPa
1.75 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N339 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0121 GPa
1.75 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Monoplex DOS Plasticizer
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0121 GPa
1.75 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Plasticizer SC
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0121 GPa

@Temperature 145 °C,
Time 2990 sec
1.75 ksi

@Temperature 293 °F,
Time 0.830 hour
cured; ASTM D412
LG Chemical NBR 6240 High Acrylonitrile Polymer
Description: NBR 6240 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6240 is a non staining, medium low mooney..
300% Modulus 0.0121 GPa
1.75 ksi
ASTM D412
Lubrizol Pellethane® 2363-80A Thermoplastic Polyurethane Elastomer
Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
300% Modulus 0.0121 GPa
1.75 ksi
ASTM D412
UBE UBEPOL VCR406 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel..
300% Modulus 0.0121 GPa
1.75 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Plasticizer SC
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0121 GPa
1.75 ksi
aged 70 hours at 300ºF
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical)
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.0121 GPa
1.75 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N339 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0121 GPa
1.75 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Monoplex DOS Plasticizer
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0121 GPa
1.75 ksi
ASTM D412
Lubrizol Estane® 2103-85AE Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in..
300% Modulus 0.0121 GPa
1.75 ksi
AdvanSource Biomaterials ChronoThane™ P Thermoplastic Polyurethane Elastomer
AdvanSource Biomaterials Corporation manufactures and markets aromatic-based ChronoThane™ P. Some characteristics that have made it attractive to medical device manufacturers include low coefficien..