PolyOne Elastamax™ XL-2155 Thermoplastic Polyolefin Elastomer (TPO (POE))

Category Polymer , Thermoplastic , Elastomer, TPE , Olefinic TPE
Manufacturer PolyOne Corporation
Trade Name Elastamax™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Elastamax™ XL-2155 Thermoplastic Polyolefin Elastomer (TPO (POE)).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance of physical properties and processability, and are an economical alternative to traditional thermoset rubber and more costly thermoplastic elastomers.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 52
52
5 sec; ASTM D2240
Tensile Strength at Break 8.76 MPa
1270 psi
510 mm/min; ASTM D412A
Tensile Stress 6.14 MPa

@Strain 100 %
891 psi

@Strain 100 %
510 mm/min; ASTM D412A
8.34 MPa

@Strain 300 %
1210 psi

@Strain 300 %
510 mm/min; ASTM D412A
Elongation at Break 370 %
370 %
510 mm/min; ASTM D412A
Tear Strength 19.3 kN/m
110 pli
Die C, 510 mm/min; ASTM D624
Compression Set 36 %

@Temperature 23.0 °C,
Time 79200 sec
36 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B
Descriptive Properties Value Comments
Additive UV Stabilizer
Features General Purpose
Forms Pellets
Generic Material TPO (POE)
Generic Name Thermoplastic Polyolefin Elastomer (TPO (POE))
Processing Method Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Construction Applications
General Purpose
Industrial Applications