Addiplast Addilene H 490 M20F Flame Retardant Polypropylene, 20% Mineral Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant , Polypropylene, Mineral Reinforced
Manufacturer Addiplast
Trade Name Addilene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addiplast Addilene H 490 M20F Flame Retardant Polypropylene, 20% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame retardant, mineral filled, with halogensInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183/A
Melt Flow 10 g/10 min
10 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 76
76
Conditioned; ISO 868
Tensile Strength at Break 28.0 MPa
4060 psi
Conditioned; ISO R 527
Elongation at Break 10 %
10 %
Conditioned; ISO R 527
Modulus of Elasticity 2.90 GPa
421 ksi
Conditioned; ISO 178
Izod Impact, Notched (ISO) 2.00 kJ/m²
0.952 ft-lb/in²
Conditioned; ISO 180/1A
Charpy Impact Unnotched 1.60 J/cm²
7.61 ft-lb/in²
Conditioned; ISO 179/IeU
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
Conditioned; ISO 179/IeA
Thermal Properties Metric English Comments
Melting Point 165 - 168 °C
329 - 334 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °C
165 °F
ISO 75-2/AF
Vicat Softening Point 153 °C
307 °F
ISO 306/A50
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Oxygen Index 27 %
27 %
ISO 4589
Glow Wire Test 960 °C
1760 °F
CEI 60695/2/1
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Conditioned; CEI 60093
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
Conditioned; CEI 60093
Dielectric Strength 43.0 kV/mm
1090 kV/in
CEI 60243-1
Comparative Tracking Index >= 600 V
>= 600 V
CEI 60112/Solution A
Users viewing this material also viewed the following: