This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66 Fiber". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.11 - 1.33 g/cc
0.0401 - 0.0480 lb/in³
Average value: 1.19 g/cc Grade Count:7
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 455 - 558 MPa
66000 - 81000 psi
Average value: 508 MPa Grade Count:3
Elongation at Break 15.0 - 45.2 %
15.0 - 45.2 %
Average value: 29.3 % Grade Count:21
Elongation at Yield 3.50 - 13.0 %
3.50 - 13.0 %
Average value: 6.83 % Grade Count:9
Tenacity 0.265 - 0.574 N/tex
3.00 - 6.50 g/denier
Average value: 0.412 N/tex Grade Count:16
Thermal Properties Metric English Comments
Melting Point 135 - 254 °C
275 - 489 °F
Average value: 237 °C Grade Count:17
Electrical Properties Metric English Comments
Electrical Resistivity 2000 - 210000 ohm-cm
2000 - 210000 ohm-cm
Average value: 38000 ohm-cm Grade Count:13