Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Silon Tabond 3045 Adhesive Resin

Category Polymer , Adhesive , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Compounding Resin
Manufacturer Silon
Trade Name Tabond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silon Tabond 3045 Adhesive Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TABOND 3045 is LLDPE modified with maleic anhydride functional groups which promote bonding with different materials like polar polymers, metals and surface treated glass.Characteristics: • Strong adhesion to aminosilane treated glass, Nylon, EVOH, PET, PBT, PC, aluminium, copper, brass and steel • Adhesion durability • Polyolefin like properties and processingInformation provided by Silon
Physical Properties Metric English Comments
Density 0.914 g/cc
0.0330 lb/in³
Melt Flow 1.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Thermal Properties Metric English Comments
Melting Point 122 °C
252 °F
DSC
Descriptive Properties Value Comments
Color White
Users viewing this material also viewed the following: