Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+8 - 1.00e+17 ohm | 1.00e+8 - 1.00e+17 ohm | Average value: 3.60e+15 ohm Grade Count:34 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | Average value: 1.00e+8 ohm Grade Count:5 |
Overview of materials for Phenolic, Novolac, Fabric Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values .. |
|||
Surface Resistance | 1.00e+8 - 8.00e+15 ohm | 1.00e+8 - 8.00e+15 ohm | Average value: 8.06e+14 ohm Grade Count:38 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Surface Resistance | 1.00e+8 - 1.00e+16 ohm | 1.00e+8 - 1.00e+16 ohm | Average value: 7.50e+15 ohm Grade Count:4 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Surface Resistance | <= 1.00e+8 ohm | <= 1.00e+8 ohm | |
Lehmann & Voss LUVOCOM® 1105-7678 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Surface Resistance | <= 1.00e+8 ohm | <= 1.00e+8 ohm | |
Lehmann & Voss LUVOCOM® 1105-8160 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Surface Resistance | <= 1.00e+8 ohm | <= 1.00e+8 ohm | |
Lehmann & Voss LUVOCOM® 1105-8167 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | |
Huntsman AVALON® 60 AE-ESD Thermoplastic Polyurethane AVALON® ESD range are soft TPUs that deliver the improved bonding strength and mechanical properties required to produce high-quality footwear on roundtable machines – specifically safety sh.. |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | |
Huntsman AVALON® 65 AK-ESD Thermoplastic Polyurethane AVALON® ESD range are soft TPUs that deliver the improved bonding strength and mechanical properties required to produce high-quality footwear on roundtable machines – specifically safety sh.. |
|||
Surface Resistance | >= 1.00e+8 ohm | >= 1.00e+8 ohm | |
Lehmann & Voss LUVOCOM® 1-8181 Polyamide 66, with carbon fiber, toughness-modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Reduced moment of inertia compared with metal parts.Elec.. |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | ASTM D257 |
LG Chemical LUCON CP-4201F Conductive Thermoplastic, Flame Retardant LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | IEC 60093 |
LG Chemical LUCON PN9009 PPS+MF Injection Molding Grade, PPS+MF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.) Motor HousingCAS No. 25212-74-2.. |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | IEC 60093 |
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP SMC 2600 is a special SMC with electrically conductive properties. Because of its conductivity, SMC 2600 is antistatic and prevents build-up of electrical charges on the surface. Despite of its cond.. |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | |
LATI Latiohm 62-09 PD01 G/20-V2HF PA6, 20% Glass Fiber Reinforced, Flame Retardant Semiconductive/dissipative product based on Polyamide 6 (PA6). Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free. Very good mechanical properties.Availabili.. |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | |
LATI Latiohm 66-08 PD02 G/35 PA66, 35% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | DIN 53482 |
Schwartz Technical Plastics LAMINEX® 2000 Cotton Fabric, Phenolic Resin Impregnated, Coarse Application: rollneck-bearings, coverts for friction rollsInformation provided by Schwartz Technical Plastics GmbH |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | DIN 53482 |
Schwartz Technical Plastics LAMINEX® 2101 Cotton Fabric, Phenolic Resin Impregnated Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | DIN 53482 |
Schwartz Technical Plastics LAMINEX® 2141 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
Surface Resistance | 1e+05 - 1.00e+8 ohm | 1e+05 - 1.00e+8 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC (Asia Pacific) Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys.. |
|||
Surface Resistance | 1.00e+8 - 1.00e+10 ohm | 1.00e+8 - 1.00e+10 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY KX09024 ACETAL COPOLYMER (Europe-Africa-Middle East) LNP* Statloy* KX09024 is a compound based on Polyacetal with reduced Resistivity. Added features include: Antistatic Properties |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | ASTM D257 |
Techmer ES Luriblend® PC CF10 TL15 FR BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE LubricantFeatures: Lubricated and Flame RetardantAppearance: BlackInformation provided.. |
|||
Surface Resistance | 1.00e+8 - 1.00e+12 ohm | 1.00e+8 - 1.00e+12 ohm | ASTM D257 |
Techmer ES Statiblend® 02056 BKN Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveAppearance: BlackTPCI# 9109116Information provided by TP Composites, Inc. |
|||
Surface Resistance | 1.00e+8 - 1.00e+11 ohm | 1.00e+8 - 1.00e+11 ohm | ASTM D257 |
Techmer ES Statiblend® PA6/6 GF10 BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: LubricantFeatures: Conductive and LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
Surface Resistance | 1.00e+8 - 1.00e+12 ohm | 1.00e+8 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics NORYL NC208 PPE+HIPS (Asia Pacific) |
|||
Surface Resistance | 1.00e+8 - 9.00e+14 ohm | 1.00e+8 - 9.00e+14 ohm | Average value: 8.27e+13 ohm Grade Count:11 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |
|||
Surface Resistance | 1.00e+8 ohm | 1.00e+8 ohm | |
LATI Latiohm 66-10 H2 CNT CE/10 PA66, 10% Mineral Fiber Reinforced, Heat Stabilized Semiconductive/dissipative product based on Polyamide 66 (PA66). Heat stabilized. Carbon nanotubes. Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame.. |
|||
Surface Resistance | 1.00e+8 - 1.00e+12 ohm | 1.00e+8 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® LC108 PC (Asia Pacific) Polycarbonate base, 8% carbon fiber reinforced, FR |