Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveAppearance: BlackTPCI# 9109116Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792
Water Absorption 0.014 %

@Time 86400 sec
0.014 %

@Time 24.0 hour
ASTM D570
Melt Flow 7.0 g/10 min

@Load 10.0 kg,
Temperature 230 °C
7.0 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85
85
ASTM D785
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Strength 26.9 MPa
3900 psi
ASTM D790
Flexural Modulus 0.965 GPa
140 ksi
ASTM D790
Izod Impact, Notched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 82.8 µm/m-°C
46.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+8 - 1.00e+12 ohm-cm
1.00e+8 - 1.00e+12 ohm-cm
ASTM D257
Surface Resistance 1.00e+8 - 1.00e+12 ohm
1.00e+8 - 1.00e+12 ohm
ASTM D257
Users viewing this material also viewed the following: