Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Luriblend® PC CF10 TL15 FR BK 10% Carbon Filled

Category Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612, Carbon Fiber Filler
Manufacturer Techmer ES
Trade Name Luriblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Luriblend® PC CF10 TL15 FR BK 10% Carbon Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE LubricantFeatures: Lubricated and Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
Water Absorption 0.080 %

@Time 86400 sec
0.080 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0035 cm/cm

@Thickness 3.17 mm
0.0035 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 108 MPa
15700 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Yield Strength 138 MPa
20000 psi
ASTM D790
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 4.27 J/cm

@Thickness 3.17 mm
8.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 19.8 µm/m-°C
11.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 147 °C
297 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
290 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+8 ohm-cm
1.00e+8 ohm-cm
ASTM D257
Surface Resistance 1.00e+8 ohm
1.00e+8 ohm
ASTM D257
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved