Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group DECAL® 666/8/2B Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group MELOPLAS® 152.7 MF Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group MELOPLAS® 183 MF Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group MELOPLAS® 2500 MF Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group MELOPLAS® 3025 MF Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group RESINOL® 87120 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Surface Resistance | 1.00e+6 - 1.00e+11 ohm | 1.00e+6 - 1.00e+11 ohm | IEC 60093 |
LG Chemical LUCON 6080EX ABS+CF Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Wide Processing RangeApplication: Carrying Cart Pipe Coating, BLU carrying TrayCAS No. 9003-56-9, 9003-54-7 and 7782-42-6Informatio.. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS (Asia Pacific) LNP STAT-LOY A3000 is a compound based on Acrylonitrile butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistatic. Also known as: STAT-LOY A |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS (Europe-Africa-Middle East) LNP* Stat-Loy* A30009 is a compound based on Acrylonitrile Butadiene resin, containing Proprietary Filler, Flame Retardant. Added features include : Permanent Antistatic, Flame retardant. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS (Asia Pacific) LNP* Stat-loy* A3000T is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS (Europe-Africa-Middle East) LNP* Stat-loy* A3000T is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: Antistat. |
|||
Surface Resistance | 1.00e+8 - 1.00e+11 ohm | 1.00e+8 - 1.00e+11 ohm | ASTM D257 |
Techmer ES Statiblend® HIPS E Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and ConductiveAppearance: Natural ColorProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly LNP* STAT-LOY* K3000SZ is a compound based on Acetal Copolymer resin. Added feature of this material is: AntiSstatic. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000SZ is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY KX95702 Acetal LNP STAT-LOY* KX95702 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY N30009 PC+ABS (Europe-Africa-Middle East) LNP* STATLOY* N30009 is a compound based on PC+ABS Blend resin containing Flame Retardant. Added features include: Permanent Antistatic, Flame Retardant. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY NX13401 PC+ABS LNP* STAT-LOY* NX13401 is a compound based on PC+ABS blend. Added features of this material include: Antistat, Flame Retardant, Excellent Release. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY PF303 PA 6 (Asia Pacific) LNP* Stat-loy* PF303 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Antistat. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | Dry; ASTM D257 |
Westlake Plastics Absylux® SD-A Acrylonitrile-Butadiene-Styrene (anti-static) Non-carbon filled anti-static material which has high impact strength, good tensile and flexural strength, and is easily machined. Available in natural or black, it can be easily thermoformed in th.. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | Dry; ASTM D257 |
Westlake Plastics Pomalux® SD-A Acetal Copolymer (anti-static) Non-carbon-filled, permanently static-dissipative material which is non-migratory and non-humidity dependent. With enhanced lubricity, POMALUX SD-A provides superior wear resistance and ease of mac.. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | Dry; ASTM D257 |
Westlake Plastics Propylux® SD-A Polypropylene (anti-static) Non-carbon-filled, permanently static-dissipative material, with good chemical resistance and mechanical properties. This material is light weight, weldable, easily machined and fabricated, availab.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IS 3396-1979 |
Amity Thermosets ATO 142 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium/hard flow Applications: Elec.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | Average value: 8.20e+10 ohm Grade Count:5 |
Overview of materials for Nylon 66/6, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group MELOPLAS® 180 MF Wood flour-reinforced, phenol-modified MF molding compound (MPF) in dark colors. High surface hardness, good mechanical strength and electrical properties, good heat resistance. Self-extinguishing .. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group RESINOL® 400 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ISO D-257 |
Premix Thermoplastics PRE-ELEC® ESD 12-000
(discontinued **) PRE-ELEC ESD 12-000 is a static dissipative thermoplastic compound based on polyacetal copolymer. The dissipative property is permanent and built into the polymer chain. The products made out of PRE.. |