Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group AMPLA® 7250 melamine-modified polyester Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group DECAL® 1760 Phenolic Glass-fiber reinforced phenolic molding compound. Very good electrical properties, good chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals an.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group DECAL® 572R Phenolic Glass-fiber reinforced phenolic molding compound. Exceptional heat resistance with regard to maintaining surface finish and mechanical properties, outstanding mechanical properties, excellent rotati.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group DECAL® 937 Phenolic Mica reinforced phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (W.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group MELOPAS® 156 MF Melamine Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group MELOPAS® 2010 MF Melamine Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group MELOPLAS® 152 MF Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group MELOPLAS® 181 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group MELOPLAS® 2500 MF Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group MELOPLAS® 3025 MF Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group RESINOL® 87120 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Surface Resistance | 1.00e+6 - 1.00e+11 ohm | 1.00e+6 - 1.00e+11 ohm | IEC 60093 |
LG Chemical LUCON 6080EX ABS+CF Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Wide Processing RangeApplication: Carrying Cart Pipe Coating, BLU carrying TrayCAS No. 9003-56-9, 9003-54-7 and 7782-42-6Informatio.. |
|||
Surface Resistance | 1.00e+8 - 1.00e+11 ohm | 1.00e+8 - 1.00e+11 ohm | ASTM D257 |
Techmer ES HiFill FR® PBT GF30 FR-S AS 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: AntistaticFeatures: Flame Retardant, Antistatic and Non-BloomingProcessing Method: Injection.. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS LNP* STAT-LOY* A30009 is a compound based on ABS. Added features of this material include: Antistatic, Flame Retardant. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS (Asia Pacific) LNP* Stat-loy* A30009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS (Europe-Africa-Middle East) LNP* Stat-Loy* A30009 is a compound based on Acrylonitrile Butadiene resin, containing Proprietary Filler, Flame Retardant. Added features include : Permanent Antistatic, Flame retardant. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific .. |
|||
Surface Resistance | 1.00e+8 - 1.00e+11 ohm | 1.00e+8 - 1.00e+11 ohm | ASTM D257 |
Techmer ES Statiblend® PA6/6 GF10 BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: LubricantFeatures: Conductive and LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY K3000Z Acetal LNP* STAT-LOY* K3000Z is a compound based on unfilled Acetal resin. Added feature of this material is: Antistat. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY KX96821 Acetal LNP STAT-LOY* KX96821 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-loy W3000 PBT LNP STAT-LOY* W3000 is a compound based on Polybutylene Terephalate resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americ.. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | Dry; ASTM D257 |
Westlake Plastics Absylux® SD-A Acrylonitrile-Butadiene-Styrene (anti-static) Non-carbon filled anti-static material which has high impact strength, good tensile and flexural strength, and is easily machined. Available in natural or black, it can be easily thermoformed in th.. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | Dry; ASTM D257 |
Westlake Plastics Propylux® SD-A Polypropylene (anti-static) Non-carbon-filled, permanently static-dissipative material, with good chemical resistance and mechanical properties. This material is light weight, weldable, easily machined and fabricated, availab.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IS 3396-1979 |
Amity Thermosets AMP 481 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Good tracking resistanceGood dielectric strengthGood electrical insulation
Applications:Switchgear components which ought to have high tracking resistanceCircuit protecting switche.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group DECAL® 152CL Phenolic Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet.. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ISO D-257 |
Premix Thermoplastics PRE-ELEC® ESD 12-000
(discontinued **) PRE-ELEC ESD 12-000 is a static dissipative thermoplastic compound based on polyacetal copolymer. The dissipative property is permanent and built into the polymer chain. The products made out of PRE.. |