Electrical Properties Metric English Comments
Surface Resistance 1.00e+14 - 1.00e+17 ohm
1.00e+14 - 1.00e+17 ohm
Average value: 8.01e+15 ohm Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an..
Surface Resistance 1.00e+8 - 1.00e+17 ohm
1.00e+8 - 1.00e+17 ohm
Average value: 3.60e+15 ohm Grade Count:34
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..
Surface Resistance 1000 - 1.00e+17 ohm
1000 - 1.00e+17 ohm
Average value: 5.23e+15 ohm Grade Count:27
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Surface Resistance 1.00e+6 - 1.00e+17 ohm
1.00e+6 - 1.00e+17 ohm
Average value: 7.79e+15 ohm Grade Count:36
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Surface Resistance 1.00e+15 - 1.00e+17 ohm
1.00e+15 - 1.00e+17 ohm
Average value: 3.70e+16 ohm Grade Count:3
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values..
Surface Resistance 1.00e+14 - 1.00e+17 ohm
1.00e+14 - 1.00e+17 ohm
Average value: 4.74e+16 ohm Grade Count:17
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor..
Surface Resistance 1.00e+14 - 1.00e+17 ohm
1.00e+14 - 1.00e+17 ohm
Average value: 1.50e+16 ohm Grade Count:34
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
Surface Resistance 100 - 1.00e+17 ohm
100 - 1.00e+17 ohm
Average value: 5.52e+15 ohm Grade Count:23
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Surface Resistance 1.00e+15 - 1.00e+17 ohm
1.00e+15 - 1.00e+17 ohm
Average value: 1.75e+16 ohm Grade Count:6
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an..
Surface Resistance 10.0 - 1.00e+17 ohm
10.0 - 1.00e+17 ohm
Average value: 6.89e+15 ohm Grade Count:37
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
Surface Resistance 1.00e+7 - 1.00e+17 ohm
1.00e+7 - 1.00e+17 ohm
Average value: 2.12e+16 ohm Grade Count:26
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
Surface Resistance 1.00e+11 - 1.00e+17 ohm
1.00e+11 - 1.00e+17 ohm
Average value: 9.84e+15 ohm Grade Count:11
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
Surface Resistance 1.00e+15 - 1.00e+17 ohm
1.00e+15 - 1.00e+17 ohm
Average value: 1.73e+16 ohm Grade Count:14
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
Surface Resistance 1.00e+12 - 1.00e+17 ohm
1.00e+12 - 1.00e+17 ohm
Average value: 5.25e+16 ohm Grade Count:4
Overview of materials for ECTFE Fluoropolymer
This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat..
Surface Resistance 10000 - 1.00e+17 ohm
10000 - 1.00e+17 ohm
Average value: 2.50e+16 ohm Grade Count:4
Overview of materials for High Density Polyethylene (HDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim..
Surface Resistance 0.200 - 1.00e+17 ohm
0.200 - 1.00e+17 ohm
Average value: 2.24e+15 ohm Grade Count:45
Overview of materials for Polyether Block Amide (PEBA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a..
Surface Resistance 1.00e+13 - 1.00e+17 ohm
1.00e+13 - 1.00e+17 ohm
Average value: 2.92e+16 ohm Grade Count:11
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Surface Resistance 1.00e+13 - 1.00e+17 ohm
1.00e+13 - 1.00e+17 ohm
Average value: 5.27e+16 ohm Grade Count:19
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m..
Surface Resistance 10000 - 1.00e+17 ohm
10000 - 1.00e+17 ohm
Average value: 4.62e+15 ohm Grade Count:27
Overview of materials for Polyimide, Thermoset Film
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr..
Surface Resistance 1.00e+13 - 1.00e+17 ohm
1.00e+13 - 1.00e+17 ohm
Average value: 1.34e+16 ohm Grade Count:16
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..