Plastcom SLOVALEN EQ 18 N PP, basic type

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVALEN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVALEN EQ 18 N PP, basic type.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesModified PE with special heat and processional stabilization. Application in extrusion of profiles and pipes, blowing of bottles and jerrycans. Delivered in black colour.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 0.943 g/cc
0.0341 lb/in³
Melt Flow 10 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 24.0 MPa
3480 psi
Elongation at Break 10 %
10 %
Tensile Modulus 0.850 GPa
123 ksi
Flexural Modulus 0.650 GPa
94.3 ksi
Charpy Impact Unnotched 3.20 J/cm²

@Temperature -20.0 °C
15.2 ft-lb/in²

@Temperature -4.00 °F
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
Charpy Impact, Notched 26.0 J/cm²

@Temperature 23.0 °C
124 ft-lb/in²

@Temperature 73.4 °F
26.0 J/cm²

@Temperature -20.0 °C
124 ft-lb/in²

@Temperature -4.00 °F
Thermal Properties Metric English Comments
Melting Point 130 °C
266 °F
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
Vicat Softening Point 75.0 °C
167 °F
B
Processing Properties Metric English Comments
Melt Temperature 180 - 230 °C
356 - 446 °F