Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styrolution Styrolux S SBC

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC
Manufacturer Styrolution
Trade Name Styrolux
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution Styrolux S SBC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Styrolux S is a new developmental, clear styrene-butadiene copolymer (SBC) designed specifically for blending with Styrolux T in order to enable high performance film extrusion and shrink film applications. As Styrolux S is blended with Styrolux T it increases the stiffness of the film and improves the storage stability of film reels (reduced natural shrinkage).Information provided by Styrolution
Physical Properties Metric English Comments
Water Absorption at Saturation 0.070 %

@Temperature 23.0 °C
0.070 %

@Temperature 73.4 °F
ISO 62
Melt Flow 11 g/10 min

@Load 5.00 kg,
Temperature 200 °C
11 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 83
83
ISO 868
Tensile Strength, Yield 2.00 MPa
290 psi
ISO 527
Elongation at Break 2.5 %
2.5 %
ISO 527
Tensile Modulus 2.90 GPa
421 ksi
ISO 527
Flexural Strength 75.0 MPa
10900 psi
ISO 178
Flexural Modulus 3.00 GPa
435 ksi
ISO 178
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Vicat Softening Point 64.0 °C

@Load 5.10 kg
147 °F

@Load 11.2 lb
50°C/h; ISO 306
70.0 °C

@Load 1.02 kg
158 °F

@Load 2.25 lb
50°C/h; ISO 306
Optical Properties Metric English Comments
Haze 1.0 %
1.0 %
ASTM D 1003
Transmission, Visible >= 90 %

@Wavelength 550 nm
>= 90 %

@Wavelength 550 nm
ASTM D 1003
Processing Properties Metric English Comments
Melt Temperature 180 - 230 °C
356 - 446 °F
ISO 294
Users viewing this material also viewed the following: