Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 203 - 250 °C | 397 - 482 °F | ISO 294 |
Styrolution Terluran® EGP-7 ABS Terluran EGP-7 is an extrusion grade with well balanced properties.UL 94 HBInformation provided by Styrolution |
|||
Melt Temperature | 203 - 275 °C | 397 - 527 °F | Injection molding/Extrusion |
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled BK 15045 PBT Description: Easy flowing injection molding grade with 15 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg timer dials, toggles, knobs, parts for thermostats, oven-door .. |