A. Schulman SCHULAMID® 6 MV14 Unreinforced Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer A. Schulman, Inc.
Trade Name SCHULAMID®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman SCHULAMID® 6 MV14 Unreinforced Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ISO 1183/1
Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.50 MPa
508 psi
ISO 527
Tensile Modulus 2.80 GPa
406 ksi
ISO 527
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.8 °C
190 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 32.2 °C
90.0 °F
ISO 75
Processing Properties Metric English Comments
Melt Temperature 240 - 275 °C
464 - 527 °F
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Drying Temperature 79.4 °C
175 °F
Dry Time 2 - 4 hour
2 - 4 hour
Predrying