Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled BK 15045 PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultradur®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled BK 15045 PBT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Easy flowing injection molding grade with 15 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg timer dials, toggles, knobs, parts for thermostats, oven-door handles, toaster housings and grills)Information provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.600 - 0.900 g/cc
0.0217 - 0.0325 lb/in³
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
Water Absorption 0.40 %
0.40 %
ISO 62
Moisture Absorption at Equilibrium 0.20 %
0.20 %
ISO 62
Viscosity Measurement 100
100
[cm<sup>3</sup>/g]; ISO 307
Linear Mold Shrinkage, Flow 0.0070 cm/cm
0.0070 in/in
ISO 2577
Linear Mold Shrinkage, Transverse 0.011 cm/cm
0.011 in/in
ISO 2577
Melt Flow 35.25 g/10 min

@Load 2.16 kg,
Temperature 250 °C
35.25 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 100 MPa
14500 psi
ISO 527-1/-2
Elongation at Break 3.5 %
3.5 %
ISO 527-1/-2
Tensile Modulus 5.50 GPa
798 ksi
ISO 527-1/-2
Charpy Impact Unnotched 3.00 J/cm²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.550 J/cm²

@Temperature 23.0 °C
2.62 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 223 °C
433 °F
ISO 11357-1/-2
Maximum Service Temperature, Air 210 °C
410 °F
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75-1/-2
Decomposition Temperature >= 290 °C
>= 554 °F
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Dielectric Constant 3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
IEC 60250
3.7

@Frequency 100 Hz
3.7

@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.0012

@Frequency 100 Hz
0.0012

@Frequency 100 Hz
IEC 60250
0.015

@Frequency 1.00e+6 Hz
0.015

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 300 V
300 V
Test Solution A; IEC 60112
Processing Properties Metric English Comments
Melt Temperature 203 - 275 °C
397 - 527 °F
Injection molding/Extrusion
Mold Temperature 60.0 - 100 °C
140 - 212 °F
Injection molding
Descriptive Properties Value Comments
Color BK 15045
Commercial Status Europe
Ignition Temperature 350°C
ASTM D1929