Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 50% Glass Fiber Reinforced
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep resistance and low moisture absorption are also characteristic of this resin.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; High Heat Resistance; High Strength; High Temperature Strength; Low Moisture AbsorptionUses: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Connectors; Housings; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools; Valves/Valve PartsInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Automotive Specifications 3M 11-0003-5762-1 Color: BK324 Black; ASTM D4000 PA121 G45 Color: BK324 Black; ASTM D4000 PA121 G45 Color: NT Natural; ASTM D4000 PPA0120 G46 A95726 AA002 CD295 GB159 MF015Z Color: BN575 Brown; ASTM D6779 PA121G45; BOSCH 9 916 365 011 Color: BK 324 Black; BOSCH 9 916 365 011 Color: NT Natural; CHRYSLER MS-DB-478 Type B CPN3567 Color: Black; FORD WSB-M4D861-A Color: BK324 Black; FORD WSB-M4D861-A Color: NT Natural; GM GMP.PPA.008 Color: BK324 Black; GM GMP.PPA.008 Color: NT Natural; GM GMW16356P-PPA-GF45 Color: BK-324 Black; GM GMW16356P-PPA-GF45 Color: NT Natural; ISO 1874 PA6T/6I/66, MH, 12-160, GF45 Color: NT Natural; TRW S-13301201 Color: BK324 BlackInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.59 g/cc
0.0574 lb/in³
Dry; ISO 1183
Filler Content 45 %
45 %
Glass Fiber
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
Linear Mold Shrinkage, Transverse 0.0010 cm/cm
0.0010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 228 MPa
33100 psi
ASTM D638
Elongation at Break 2.1 %
2.1 %
ASTM D638
Tensile Modulus 17.2 GPa
2490 ksi
ASTM D638
Flexural Strength 294 MPa
42600 psi
ASTM D790
Flexural Modulus 13.8 GPa
2000 ksi
ASTM D790
Shear Strength 91.7 MPa
13300 psi
ASTM D732
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 310 °C
590 °F
Peak; Dry; ASTM D3418
310 °C
590 °F
Dry; ISO 11357-3
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+15 ohm-cm
2.00e+15 ohm-cm
ASTM D257
Dielectric Constant 4.5

@Frequency 1.00e+6 Hz
4.5

@Frequency 1.00e+6 Hz
ASTM D150
4.9

@Frequency 60.0 Hz
4.9

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 23.0 kV/mm

@Thickness 3.20 mm
584 kV/in

@Thickness 0.126 in
ASTM D149
Dissipation Factor 0.0090

@Frequency 60.0 Hz
0.0090

@Frequency 60.0 Hz
ASTM D150
0.021

@Frequency 1.00e+6 Hz
0.021

@Frequency 1.00e+6 Hz
ASTM D150
Arc Resistance 125 sec
125 sec
ASTM D495
Comparative Tracking Index 550 V
550 V
UL 746
Processing Properties Metric English Comments
Rear Barrel Temperature 304 - 318 °C
579 - 604 °F
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Melt Temperature 321 - 343 °C
610 - 649 °F
Mold Temperature 135 °C
275 °F
Drying Temperature 120 °C

@Time 16200 sec
248 °F

@Time 4.50 hour
Moisture Content <= 0.045 %
<= 0.045 %
Descriptive Properties Value Comments
Additive Heat Stabilizer
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black; Natural
Form Pellets
Processing Technique Injection Molding
RoHS Compliance RoHS Compliant
Copyright © lookpolymers.com All Rights Reserved