Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 12.8 - 32.2 °C | 55.0 - 90.0 °F | |
PolyOne Versaflex™ CL2000X Thermoplastic Elastomer (TPE) Versaflex™ CL2000X is an ultra-soft TPE designed for use in injection molding applications where exceptional clarity and an extremely soft feel are desired. - Tactile Feel - Ultra-Soft - Water Clar.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
PolyOne Versaflex™ CL2050 Thermoplastic Elastomer (TPE) Versaflex™ CL2050 is an easy processing compound designed for use in applications where clarity and enhanced heat resistance are required. New Product. Commercial specifications have not been estab.. |
|||
Mold Temperature | 12.8 - 32.2 °C | 55.0 - 90.0 °F | |
PolyOne Versaflex™ FFC 2882-87 Thermoplastic Elastomer (TPE) Versaflex™ FFC 2882-87 is designed to pass several fatty food extraction conditions identified in EU Directive 2002/72/EC, FDA 21 CFR 177.2600, and GB 4806.1-94. Versaflex™ FFC 2882-87 will also o.. |
|||
Mold Temperature | 12.8 - 32.2 °C | 55.0 - 90.0 °F | |
PolyOne Versaflex™ HC 2110-57B Thermoplastic Elastomer (TPE) Versaflex™ HC 2110-57B is a TPE designed for use in the healthcare industry offering low stiction and good compression set. New Product. Commercial specifications have not been established. - Bonds.. |
|||
Mold Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | |
PolyOne Versaflex™ OM 2262 Thermoplastic Elastomer (TPE) Versaflex™ OM 2262 is a performance overmolding grade with general FDA compliance. This product is designed for both insert and two-shot molding onto Eastman Tritan™ copolyester as well as ABS, PC.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
PolyOne Versollan™ RU 2205-1 Thermoplastic Elastomer (TPE) Versollan™ RU 2205-1 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
PolyOne Versollan™ RU 2205-9 Thermoplastic Elastomer (TPE) Versollan™ RU 2205-9 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
Northstar Polymers MCP-V40A Polyurethane Gel MCP-V40A is a polyurethane gel formulation specifically designed for padding and cushioning applications, where low rebound property of the material is critical. This viscoelastic polymer is a two.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
Northstar Polymers MPC-W44A Polyurethane Gel MPC-W44A is a polyurethane gel formulation specifically designed for padding and cushioning application that requires Shore Durometer OOO scale hardness. Produces good rebound characteristics and g.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
Northstar Polymers MPP-A47A Liquid Castable Polyurethane MPP-A47A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
Northstar Polymers MPP-A50A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
Northstar Polymers MPP-A60A Liquid Castable Polyurethane MPP-A60A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
PolyOne Dynaflex™ D3204-1000-03 Thermoplastic Elastomer (TPE) Dynaflex™ D3204-1000-03 is an easy processing TPE designed for general purpose applications and is suitable for injection molding, extrusion, blow molding, and thermoforming processes. - Dry Feel -.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
PolyOne Dynaflex™ D3226-1000-03 Thermoplastic Elastomer (TPE) Dynaflex™ D3226-1000-03 is an easy processing TPE designed for general purpose applications. It is suitable for injection molding, extrusion, blow molding and thermoforming processes. - Dry Feel - .. |
|||
Mold Temperature | 15.6 - 32.2 °C | 60.1 - 90.0 °F | |
PolyOne Dynalloy™ OBC8000-T05 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8000-T05 is an ultra-soft TPE utilizing the unique rubber properties of Dows INFUSE™ Olefin Block Copolymers. This product is designed for injection molding applications where excepti.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
Northstar Polymers GK-7 Low Viscosity Polyurethane Gel Cast This material is formulated for production of thin polyurethane gel film or parts. The low viscosity property of the mixed component enables the user to cast this into a thin layer without entrappi.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
Northstar Polymers MCG-1 OOO Scale Microcellular Gel Elastomer MCG-1 is formulated for making extremely soft products. MCG-1 has unique structure for this class of material. The cured product will be slightly foamed and give a very soft touch, yet faster resp.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
Northstar Polymers MPP-A65A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
Northstar Polymers SAI-1 Low Viscosity Variable Ratio Polyurethane Gel SAI-1 is custom formulated polyurethane gel material to yield very soft elastomer gel material from low viscosity components at room temperature. This material is variable mixing ratio so that the .. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
MRC Polymers MAXTELâ„¢ 600T10-BK TPO, 10% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
MRC Polymers MAXTELâ„¢ 600T25 TPO, 25% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
MRC Polymers MAXTELâ„¢ 600T30IM TPO, 30% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityImpact ModifiedCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Pol.. |