Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styrolution Polystyrol 495 F GR 2 PS

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Styrolution
Trade Name Polystyrol
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution Polystyrol 495 F GR 2 PS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polystyrol 495 F is a high impact polystyrene with a good heat resistance and high stiffness.Applications: Consumer electronics; TV-front and back; chassis for VCR and CD player. Household: internal parts of vacuum cleaners; refrigerator parts; drawers; audio- and video cassettes; printer housings, keyboards, computers, copier parts.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Physical Properties Metric English Comments
Density 1.028 g/cc
0.03714 lb/in³
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
ISO 62
Moisture Absorption at Equilibrium <= 0.10 %
<= 0.10 %
23°C/50% RH; ISO 62
Melt Flow 9.766 g/10 min

@Load 5.00 kg,
Temperature 200 °C
9.766 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Mechanical Properties Metric English Comments
Ball Indentation Hardness 74.0 MPa

@Load 36.5 kg,
Time 30.0 sec
10700 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Tensile Strength, Yield 26.0 MPa
3770 psi
50 mm/min; ISO 527-1/-2
Elongation at Break 40 %
40 %
Nominal, 50mm/min; ISO 527-1/-2
Elongation at Yield 1.5 %
1.5 %
50 mm/min; ISO 527-1/-2
Tensile Modulus 2.00 GPa
290 ksi
ISO 527-1/-2
Flexural Strength 40.0 MPa
5800 psi
ISO 178
Flexural Modulus 2.10 GPa
305 ksi
ASTM D790
Izod Impact, Notched 1.80 J/cm
3.37 ft-lb/in
ASTM D256
Charpy Impact Unnotched <= 13.0 J/cm²

@Temperature -30.0 °C
<= 61.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
<= NB

@Temperature 23.0 °C
<= NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °C
192 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ISO 75-1/-2
Vicat Softening Point 88.5 °C
191 °F
VST/B/50; ISO 306
98.0 °C
208 °F
VST/A/50; ISO 306
Flammability, UL94 HB

@Diameter 1.60 mm
HB

@Diameter 0.0630 in
IEC 60695-11-10
HB

@Diameter 3.00 mm
HB

@Diameter 0.118 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
IEC 60093
Dielectric Constant 2.5

@Frequency 1.00e+6 Hz
2.5

@Frequency 1.00e+6 Hz
IEC 60250
2.5

@Frequency 100 Hz
2.5

@Frequency 100 Hz
IEC 60250
Dielectric Strength 155 kV/mm
3940 kV/in
K20/P50; IEC 60243-1
Processing Properties Metric English Comments
Melt Temperature 180 - 260 °C
356 - 500 °F
Injection molding
Mold Temperature 10.0 - 60.0 °C
50.0 - 140 °F
Injection Molding
Descriptive Properties Value Comments
Color Natural
Commercial Status Europe
Primary Processing Technique Injection Molding
Surface Gloss 45
Skalenteile
Copyright © lookpolymers.com All Rights Reserved