Material Notes:
Type: Estane® S360D is a Shore 63D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ASTM D2240
Tensile Strength, Ultimate 42.2 MPa
6120 psi
ASTM D412
Tensile Strength, Yield 21.6 MPa
3130 psi
at 100% elongation; ASTM D412
35.3 MPa
5120 psi
at 300% elongation; ASTM D412
Elongation at Break 400 %
400 %
ASTM D412
Tear Strength 216 kN/m
1230 pli
Die C; ASTM D624
Abrasion 30
30
mm<sup>3</sup> loss; ISO 4649
Compression Set 20 %

@Temperature 23.0 °C,
Time 79200 sec
20 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
40 %

@Temperature 70.0 °C,
Time 79200 sec
40 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Vicat Softening Point 123 °C
253 °F
ASTM D1525
Processing Properties Metric English Comments
Feed Temperature 200 - 215 °C
392 - 419 °F
Nozzle Temperature 215 - 230 °C
419 - 446 °F
Mold Temperature 10.0 - 40.0 °C
50.0 - 104 °F
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Injection Pressure 12.4 - 16.5 MPa
1800 - 2400 psi
Hold Pressure 8.96 - 13.1 MPa
1300 - 1900 psi
Back Pressure 0.207 - 0.552 MPa
30.0 - 80.0 psi
Cycle Time - Injection 25 - 30 sec
25 - 30 sec
Screw Speed 160 - 200 rpm
160 - 200 rpm
Descriptive Properties Value Comments
Injection time (s) 12-18
Metering Zone 210-225°C