Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyester Alloy , Polyester, TP
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for ABS/Polyester Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.07 - 1.58 g/cc
0.0387 - 0.0571 lb/in³
Average value: 1.22 g/cc Grade Count:22
Water Absorption 0.0140 - 0.150 %
0.0140 - 0.150 %
Average value: 0.0877 % Grade Count:7
Linear Mold Shrinkage 0.00100 - 0.0140 cm/cm
0.00100 - 0.0140 in/in
Average value: 0.00636 cm/cm Grade Count:17
Melt Flow 11.0 - 35.0 g/10 min
11.0 - 35.0 g/10 min
Average value: 20.1 g/10 min Grade Count:7
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85.0 - 117
85.0 - 117
Average value: 102 Grade Count:12
Tensile Strength, Ultimate 26.5 - 41.4 MPa
3840 - 6000 psi
Average value: 35.1 MPa Grade Count:4
Tensile Strength, Yield 21.4 - 117 MPa
3100 - 17000 psi
Average value: 51.5 MPa Grade Count:20
Elongation at Break 3.30 - 100 %
3.30 - 100 %
Average value: 42.2 % Grade Count:19
Flexural Yield Strength 49.0 - 151 MPa
7110 - 21900 psi
Average value: 74.3 MPa Grade Count:21
Flexural Modulus 0.238 - 10.4 GPa
34.5 - 1510 ksi
Average value: 2.79 GPa Grade Count:22
Izod Impact, Notched 0.374 - 7.47 J/cm
0.700 - 14.0 ft-lb/in
Average value: 1.94 J/cm Grade Count:22
Thermal Properties Metric English Comments
CTE, linear 30.0 - 103 µm/m-°C
16.7 - 57.0 µin/in-°F
Average value: 68.7 µm/m-°C Grade Count:7
Deflection Temperature at 0.46 MPa (66 psi) 86.0 - 202 °C
187 - 396 °F
Average value: 122 °C Grade Count:14
Deflection Temperature at 1.8 MPa (264 psi) 78.0 - 214 °C
172 - 417 °F
Average value: 97.0 °C Grade Count:16
Vicat Softening Point 88.0 - 104 °C
190 - 219 °F
Average value: 93.5 °C Grade Count:5
Flammability, UL94 HB - 5VA
HB - 5VA
Grade Count:18
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 - 1.00e+16 ohm-cm
1.00e+15 - 1.00e+16 ohm-cm
Average value: 7.75e+15 ohm-cm Grade Count:4
Surface Resistance 1.00e+14 - 1.00e+16 ohm
1.00e+14 - 1.00e+16 ohm
Average value: 6.70e+15 ohm Grade Count:3
Dielectric Strength 17.7 - 29.5 kV/mm
450 - 750 kV/in
Average value: 26.1 kV/mm Grade Count:4
Processing Properties Metric English Comments
Mold Temperature 10.0 - 80.0 °C
50.0 - 176 °F
Average value: 58.2 °C Grade Count:5
Users viewing this material also viewed the following: