Wanhua Chemical Wanthane® WHT-7185 Polycaprolactone Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-7185 Polycaprolactone Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Higher mechanical strength, good hydrolytic stability & chemical resistance, weather resistance, heat & fungus resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
ASTM D2240
Tensile Strength 35.0 MPa
5080 psi
ASTM D412
Elongation at Break 350 %
350 %
ASTM D412
100% Modulus 0.00800 GPa
1.16 ksi
ASTM D412
300% Modulus 0.0230 GPa
3.34 ksi
ASTM D412
Tear Strength 100 kN/m
571 pli
ASTM D624
Processing Properties Metric English Comments
Processing Temperature 190 - 210 °C
374 - 410 °F