Specialties: High transparencyLow neck-inNucleated typeApplications: Suitable for T-die,Water and Air blown process Processing: Shrink bags (Water) Pouch ( Air blown) Information provided by UBE.
Physical Properties Metric English Comments
Relative Viscosity 3.8 - 3.98 cP
3.8 - 3.98 cP
96% H2SO4
4.1 - 4.3 cP
4.1 - 4.3 cP
98% H2SO4
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 540 %
540 %
Film Elongation at Break, TD 560 %
560 %
Secant Modulus, MD 0.210 GPa
30.5 ksi
Secant Modulus, TD 0.230 GPa
33.4 ksi
Coefficient of Friction, Dynamic 0.39
0.39
Coefficient of Friction, Static 0.49
0.49
Film Tensile Strength at Break, MD 42.0 MPa
6090 psi
Film Tensile Strength at Break, TD 40.0 MPa
5800 psi
Thermal Properties Metric English Comments
Melting Point 187 - 197 °C
369 - 387 °F
Optical Properties Metric English Comments
Haze 10.4 %
10.4 %
Gloss 120 %
120 %
Processing Properties Metric English Comments
Processing Temperature 190 - 210 °C
374 - 410 °F
C1
220 - 230 °C
428 - 446 °F
C2
230 - 240 °C
446 - 464 °F
C3
230 - 240 °C
446 - 464 °F
C4
240 - 250 °C
464 - 482 °F
AD
240 - 250 °C
464 - 482 °F
CF
240 - 250 °C
464 - 482 °F
D1- D4
Descriptive Properties Value Comments
Degree of Curling 7 Mm