Material Notes:
Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Tensile Strength 30.0 MPa
4350 psi
ASTM D412
Elongation at Break 400 %
400 %
ASTM D412
100% Modulus 0.0110 GPa
1.60 ksi
ASTM D412
300% Modulus 0.0250 GPa
3.63 ksi
ASTM D412
Tear Strength 95.0 kN/m
542 pli
ASTM D624
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
Processing Properties Metric English Comments
Processing Temperature 190 - 210 °C
374 - 410 °F