Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 170 - 185 °C | 338 - 365 °F | Activation Temperature |
PolyOne Geon™ Vinyl Wire & Cable EAS81A Polyvinyl Chloride, Flexible (PVC, Flexible) Geon© EAS81A is a Vinyl Foam Concentrate for Wire and Cable Extrusion. This product is an exothermic type blowing agent intended to be used with a wide range of Wire and Cable Vinyl formulations to.. |
|||
Processing Temperature | 170 - 220 °C | 338 - 428 °F | |
PolyChem Alloy 6004 Talc Nucleator Talc nucleator products are additive masterbatch concentrates designed for the nucleation of both commodity and engineering thermoplastic resins. Talc Nucleators typically contain 40 to 60 % by weig.. |
|||
Processing Temperature | 170 - 180 °C | 338 - 356 °F | Plasticizing Zone; Coextrusion with polyamide |
Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength.. |
|||
Processing Temperature | 170 - 180 °C | 338 - 356 °F | Collar Temperature |
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Processing Temperature | 170 - 230 °C | 338 - 446 °F | |
PolyChem Alloy 5006 Talc Nucleator Talc nucleator products are additive masterbatch concentrates designed for the nucleation of both commodity and engineering thermoplastic resins. Talc Nucleators typically contain 40 to 60 % by weig.. |
|||
Processing Temperature | 170 - 185 °C | 338 - 365 °F | Mixture Zone |
Petroquimica Triunfo Trithene® TX 3003 LDPE - Shrink Wrap Film The Trithene® TX 3003 resin is a low-density polyethylene (LDPE) with high molecular weight, presenting excellent mechanical properties. The product provided elevated gloss and transparency, adding.. |
|||
Processing Temperature | 170 - 185 °C | 338 - 365 °F | Molding temperature |
Cookson Group Plaskon® 1002 Conventional Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low cost, low stress, conventional molding compound recommended for high volume commodity-type packages that house simple linea.. |
|||
Processing Temperature | 170 - 185 °C | 338 - 365 °F | Molding temperature |
Cookson Group Plaskon® S-7LA Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low alpha emission molding compound designed for packaging stress-sensitive memory devices. It offers an alpha par.. |
|||
Processing Temperature | 170 - 185 °C | 338 - 365 °F | Molding temperature |
Cookson Group Plaskon® SMT-B-1 LAS (146.408) Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for grid arrays (BGA/LGA) requiring low alpha particle count. It is formulated .. |
|||
Processing Temperature | 170 - 185 °C | 338 - 365 °F | Molding temperature |
Cookson Group Plaskon® ULS-12 Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A state-of-the-art, ultra low stress epoxy encapsulant designed for packaging large, stress-sensitive DIPs, PLCCs and QFPs. It i.. |
|||
Processing Temperature | 170 - 185 °C | 338 - 365 °F | Molding temperature |
Cookson Group Plaskon® ULS-12LA Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An ultra low stress, low alpha emission molding compound designed for packaging stress-sensitive memory devices such as TSOPs and.. |
|||
Processing Temperature | 170 °C | 338 °F | Cure Schedule: 5/20 min @ 170/220°C |
Huntsman HZ 3365 Special Hardener Mix Ratio with 100 phr GT 6097 or GT 6609 US is 25.Comments/Applications: Hardener in solution for heat curing systems useful in can and coil applications. *Mix ratio with GT 6097 or GT 6609 US.Da.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | thermoforming temperature |
Lucite International XL Sanitary Ware Acrylic Sheet Lucite® XL continuous-cast cross-linked acrylic sheet is specially formulated for deep-draw thermoforming. It is used primarily for production of spas.Benefits: Smooth surface; Infinite colors an.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | Metering Temperature, Extrusion |
Stellarchem LP-870 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | Metering Temperature, Extrusion |
Stellarchem MP-845B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Processing Temperature | 170 - 210 °C | 338 - 410 °F | Extrusion Temp |
Total LLDPE LL 1820 Linear Low Density Polyethylene - Blown Film LL 1820 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 can be processed at high outpu.. |
|||
Processing Temperature | 170 - 240 °C | 338 - 464 °F | |
Zhejiang Juner PP8 PP For Automotive Parts Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | |
Wanhua Chemical Wanthane® WHT-1565 Polyester Based TPU Plasticizer free, excellent abrasion & slip resistance, low temperature flexibility, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Processing Temperature | 170 - 210 °C | 338 - 410 °F | |
ELASTO UK Dryflex® 402801S SBS Based Material, 80A Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Processing Temperature | 170 - 200 °C | 338 - 392 °F | Films Die Head |
EMS-Griltech Griltex® D 1309E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 170 °C | 338 °F | Cure Measuring Temperature |
Daikin DAI-EL G-701 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: General purpose with excellent compression set.Information provided by.. |
|||
Processing Temperature | 170 °C | 338 °F | Cure Measuring Temperature |
Daikin DAI-EL G-716 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Minimal compression set and fast vulcanization.Information provided by.. |
|||
Processing Temperature | 170 °C | 338 °F | Cure Measuring Temperature |
Daikin DAI-EL G-752 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Processing Temperature | 170 °C | 338 °F | Cure Measuring Temperature |
Daikin DAI-EL G-783 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Fast vulcanization, for complex shapes.Information provided by Daikin .. |
|||
Processing Temperature | 170 °C | 338 °F | Cure Measuring Temperature |
Daikin DAI-EL G-551 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 69% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Products with excellent balance of.. |
|||
Processing Temperature | 170 - 240 °C | 338 - 464 °F | Injection molding |
BASF Elastollan 1154 D FHF TPUR Flame Retardant Halogen Free Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Processing Temperature | 170 - 240 °C | 338 - 464 °F | Injection molding |
BASF Elastollan 1198 A TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Processing Temperature | 170 - 300 °C | 338 - 572 °F | |
Asahi Kasei ASACLEAN UP Sun Plastech Purging Compound Specifically for Polypropylene, Purging compound for plastic injection molding machines and extrudersProcessing Notes: Purging to and from polypropylene based resins within temperature rangeInformat.. |