Processing Properties Metric English Comments
Processing Temperature 200 - 235 °C
392 - 455 °F
Barrel Temperature
SABIC PP 412MK49 Polypropylene Impact Copolymer for Injection Molding
Product Description: PP 412MK49 is specially developed for producing injection molded articles. This grade contains an antistatic & nucleating agents. It has medium flow properties, good impact r..
Processing Temperature <= 200 °C
<= 392 °F
To prevent fiber degradation.
North Wood Plastics 60 HDPE + UNIFILL (20% Wood Fiber)
Data provided by North Wood Plastics, Inc. UNIFILL-60 is a general purpose polyolefin compound compatible in both PP and HDPE. It is a masterbatch with 60% high quality pine wood flour filler. It..
Processing Temperature 200 °C
392 °F
Center barrel temperature
Rotuba MH Cellulose Acetate
Property values at 50% RH.Data provided by the manufacturer.
Processing Temperature 200 - 315 °C
392 - 599 °F
Average value: 235 °C Grade Count:42
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported ..
Processing Temperature 200 °C
392 °F
mass temp
Lehmann & Voss LUVOCOM® 80/TF/18/GY Polyacetal-copolymer, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Processing Temperature 200 °C
392 °F
mass temp
Lehmann & Voss LUVOCOM® 80/TF/18/SI/2/BK Polyacetal-copolymer, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Processing Temperature 200 °C
392 °F
mass temp
Lehmann & Voss LUVOCOM® 80-7112/BK Polyacetal-copolymer, with glass fiber and carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
Processing Temperature 200 °C
392 °F
mass temp
Lehmann & Voss LUVOCOM® 80-7718 Polyacetal-copolymer, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Processing Temperature 200 °C
392 °F
mass temp
Lehmann & Voss LUVOCOM® 80-8444 Polyacetal-copolymer, unreinforced
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.dynamic stressReduced moment of inertia compared with metal parts.Isotropic shrinkage character..
Processing Temperature 200 °C
392 °F
recommended
ICO Polymers ICOFLOâ„¢ 510-5056 500 Micron LDPE Powder
Description: ICOFLO 510-5056 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Processing Temperature 200 °C
392 °F
recommended
ICO Polymers ICOFLOâ„¢ 510-5057 80 Micron LDPE Powder
Description: ICOFLO 510-5057 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Processing Temperature 200 - 240 °C
392 - 464 °F
injection, multi-filament
IRPC Polimaxx Polene 1100RC Polypropylene Homopolymer
CHARACTERISTICS: HIGH FLOW, GOOD STIFFNESS, GOOD PROCESSABILITY, GOOD MELT STABILITYAPPLICATIONS: INJECTION MOLDING FOR THIN WALL PARTS, HOUSE WARES EXTRUSION COATING FOR COATED WOVEN BAGS AND TARPA..
Processing Temperature 200 - 260 °C
392 - 500 °F
IRPC Polimaxx Polene R1760 High Density Polyethylene
CHARACTERISTICS: HIGH IMPACT STRENGTH, EXCELLENT SURFACE APPEARANCE, GOOD RIGIDITY CONTAIN UV STABILIZER ADDITIVEAPPLICATIONS: INJECTION MOLDING FOR CRATES, TRAYS, CASES, INDUSTRIAL PARTS, BINS, LAR..
Processing Temperature 200 - 220 °C
392 - 428 °F
Metering Temperature, Extrusion
Stellarchem 475-860N TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Processing Temperature 200 - 220 °C
392 - 428 °F
Metering Temperature, Extrusion
Stellarchem HP-930NC-HD TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Processing Temperature 200 - 220 °C
392 - 428 °F
Metering Temperature, Extrusion
Stellarchem LP-880 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Processing Temperature 200 °C
392 °F
Metering Temperature
SK Chemicals SKYTHANE® X595A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Processing Temperature 200 - 220 °C
392 - 428 °F
C1
UBE 1026B1 Nylon 6 Homopolymer Film
Specialties: Nucleated (High viscosity) Processing: T-die, Air blownApplications: General applicationsInformation provided by UBE.
Processing Temperature 200 - 210 °C
392 - 410 °F
C2
UBE 7034B Nylon 6/12 Copolymer Film
Specialties: High transparencyGood thermoform-abilityLow W.V.T.R High shrink-abilityLower extrusion temperatureProcessing: Best match for co-extrusion with EVOH resins.Typical Applications: Cereal ..
Processing Temperature 200 - 260 °C
392 - 500 °F
mass temperature
Borealis HK030U Polypropylene Compound
HK030U is a special low viscosity polypropylene compound developed to fit the production of PP-GF composites in the direct LFT compression and injection molding process as well as in combination wit..
Processing Temperature 200 - 250 °C
392 - 482 °F
mass temperature on double belt presses
Borealis HK060AE Polypropylene Homopolymer
HK060AE is a special low viscosity polypropylene homopolymer compound developed to fit the production of glass matt reinforced thermoplastics. This material is also suitable as base resin for the pr..
Processing Temperature 200 - 240 °C
392 - 464 °F
Eurotec® Tecolen® CP20 BK EC PPCP, conductive, black
Information provided by Eurotec®
Processing Temperature 200 - 240 °C
392 - 464 °F
Eurotec® Tecolen® CP20 MF20 NL XA70 PPCP, 20% mineral filled, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
Processing Temperature 200 - 240 °C
392 - 464 °F
Eurotec® Tecolen® CP30 GR20 NL PPCP, 20% glass fiber reinforced, natural, high flow grade
Information provided by Eurotec®
Processing Temperature 200 °C
392 °F
Gate Temperature; Extrusion
Alliance Polymers Viprene™ G80A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G80A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Processing Temperature 200 - 205 °C
392 - 401 °F
Injection
Alliance Polymers Zythane™ 4080A Thermoplastic Polyurethane Elastomer
Zythane™ 4080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Processing Temperature 200 °C
392 °F
Hopper Throat
BASF Ultraform® N2320 U035 POM
Description: Is a POM, UV-stabilized injection-molding grade.Information provided by BASF
Processing Temperature 200 °C
392 °F
Hopper Throat
BASF Ultraform® N2640 E4 POM
Description: Is a POM + MBS, elastomer-modified injection-molding grade with high toughness and high weld line strength.Information provided by BASF
Processing Temperature 200 °C
392 °F
Hopper Throat
BASF Ultraform® N2640 Z2 POM + PUR
Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS..
Processing Temperature 200 - 220 °C
392 - 428 °F
Wanhua Chemical Wanthane® WHT-1164 Polyester Based TPU
Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd.
Copyright © lookpolymers.com All Rights Reserved