Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 140 - 160 °C | 284 - 320 °F | Collar Temperature |
Solvay Specialty Polymers Cogegum® GFR/325 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Processing Temperature | 140 - 210 °C | 284 - 410 °F | Average value: 170 °C Grade Count:11 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |
|||
Processing Temperature | 140 - 160 °C | 284 - 320 °F | Compression moulding, matched metal die |
Menzolit Menzolit® HPC 1300 Unsaturated Polyester UP HPC 1300 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc.. |
|||
Processing Temperature | 140 °C | 284 °F | Mixing Roll |
SK Chemicals SKYTHANE® CR180A Calendaring Series, Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Processing Temperature | 140 - 180 °C | 284 - 356 °F | Films Die Head |
EMS-Griltech Griltex® 2A Copolyamide Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 140 - 170 °C | 284 - 338 °F | Lamination Adhesive |
EMS-Griltech Griltex® D 1619E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 140 °C | 284 °F | curing temp. |
Arlon 0.008" (0.2032 mm) Thermabond® E-35 Uncured Silicone (99730N008) 0.008 in., ±0.001 (0.2 mm, ±0.03) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.008 in ±0.001(0.2 mm ± 0.03). T.. |
|||
Processing Temperature | >= 140 °C | >= 284 °F | |
Bulk Molding Compounds BMC 665 Mineral Filled, Glass Reinforced Polyester BMC 665 molding compound is a mineral filled, glass reinforced polyester molding compound suitable for compression, transfer or stuffer injection molding. It is characterized by good moldability, o.. |
|||
Processing Temperature | 140 - 230 °C | 284 - 446 °F | Average value: 194 °C Grade Count:32 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |
|||
Processing Temperature | 140 °C | 284 °F | Suggested baking time at this temperature is 0.5-2 hr. |
Von Roll Isola IMI Varnish 73517 Solventless Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: 30°C. Usag.. |