Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 170 - 220 °C | 338 - 428 °F | |
PolyChem Alloy 4005 Talc Nucleator Talc nucleator products are additive masterbatch concentrates designed for the nucleation of both commodity and engineering thermoplastic resins. Talc Nucleators typically contain 40 to 60 % by weig.. |
|||
Processing Temperature | 170 - 180 °C | 338 - 356 °F | Collar Temperature |
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Processing Temperature | 170 - 230 °C | 338 - 446 °F | |
PolyChem Alloy PolyBlaz 7525PM An Antimicrobial Agent Masterbatch. |
|||
Processing Temperature | 170 - 220 °C | 338 - 428 °F | Average value: 194 °C Grade Count:5 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum.. |
|||
Processing Temperature | 170 - 185 °C | 338 - 365 °F | Molding temperature |
Cookson Group Plaskon® 435 Mineral Filled Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.Combines exceptional reliability with wide molding process latitude. This material is designed to encapsulate a variety of semic.. |
|||
Processing Temperature | 170 - 185 °C | 338 - 365 °F | Molding temperature |
Cookson Group Plaskon® 3400 Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A reduced-stress epoxy molding compound for the encapsulation of a variety of semiconductor devices ranging from small lead count.. |
|||
Processing Temperature | 170 - 185 °C | 338 - 365 °F | Molding temperature |
Cookson Group Plaskon® ULS-12HLG Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A state-of-the-art, ultra low stress epoxy encapsulant designed for packaging large, stress-sensitive DIPs, PLCCs and QFPs. It i.. |
|||
Processing Temperature | 170 - 250 °C | 338 - 482 °F | |
IRPC Polimaxx Polene 2500H Polypropylene Block Copolymer CHARACTERISTICS: EXCELLENT HIGH IMPACT, HIGH TOUGHNESS GOOD EXTRUDABILITYAPPLICATIONS: SHEET / BLOW MOLD EXTRUSION AND INJECTION MOLDING FOR CORRUGATE SHEETS, SHEETS FOR FILE, HOUSEWARES, CONTAINERS.. |
|||
Processing Temperature | 170 - 200 °C | 338 - 392 °F | |
IRPC Polimaxx Polene GM2860 High Density Polyethylene CHARACTERISTICS: HIGH IMPACT STRENGTH, GOOD PROCESSABILITY, HIGH STIFFNESSAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, LUBRICANT BOTTLES COSMETIC BOTTLES, ONE-WAY BOTT.. |
|||
Processing Temperature | 170 - 200 °C | 338 - 392 °F | Forming |
KYDEX® 5555 Low Heat Release Aviation Thermoforming Sheet Features:Over two hundred colors and eight thicknesses availableChemical resistantMeets flamespread and smoke density requirements for mass transitSuggested Applications:Seat partsBulkhead laminates.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | Metering Temperature, Extrusion |
Stellarchem 8075 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | Metering Temperature, Extrusion |
Stellarchem GP-930 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | Metering Temperature, Extrusion |
Stellarchem LP-870 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Processing Temperature | 170 - 240 °C | 338 - 464 °F | |
Zhejiang Juner PP8 PP For Automotive Parts Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 170 - 210 °C | 338 - 410 °F | |
ELASTO UK Dryflex® 400701S SBS Based Material, 70A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Processing Temperature | 170 - 210 °C | 338 - 410 °F | |
ELASTO UK Dryflex® 402501S SBS Based Material, 50A Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Processing Temperature | 170 - 200 °C | 338 - 392 °F | Films Die Head |
EMS-Griltech Griltex® D 1309E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 170 °C | 338 °F | Cure Measuring Temperature |
Daikin DAI-EL G-671 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 67% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Excellent low-temperature sealing .. |
|||
Processing Temperature | 170 °C | 338 °F | Cure Measuring Temperature |
Daikin DAI-EL G-701 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: General purpose with excellent compression set.Information provided by.. |
|||
Processing Temperature | 170 °C | 338 °F | Cure Measuring Temperature |
Daikin DAI-EL G-704 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Processing Temperature | 170 °C | 338 °F | Cure Measuring Temperature |
Daikin DAI-EL G-716 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Minimal compression set and fast vulcanization.Information provided by.. |
|||
Processing Temperature | 170 °C | 338 °F | Cure Measuring Temperature |
Daikin DAI-EL G-752 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Processing Temperature | 170 °C | 338 °F | Cure Measuring Temperature |
Daikin DAI-EL G-783 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Fast vulcanization, for complex shapes.Information provided by Daikin .. |
|||
Processing Temperature | 170 - 210 °C | 338 - 410 °F | |
Eurotec® Tecoform® PO20 NL IL POM, impact modified, natural Information provided by Eurotec® |
|||
Processing Temperature | >= 170 °C | >= 338 °F | in blown film extrusion |
Arkema Group LOTRYL® Bestpeel 2407 Copolymer Ethylene - Methyl Acrylate LOTRYL® Bestpeel 2407 is a ready-to-use thermoplastic composition designed to make peelable heat seal layers onto various substrates. The base resin is a random copolymer of ethylene and methyl acr.. |
|||
Processing Temperature | 170 - 240 °C | 338 - 464 °F | Injection molding |
BASF Elastollan 1154 D FHF TPUR Flame Retardant Halogen Free Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Processing Temperature | 170 - 240 °C | 338 - 464 °F | Injection molding |
BASF Elastollan 1198 A TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |