Wanhua Chemical Wanthane® WHT-1295 Polyester Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-1295 Polyester Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 96
96
ASTM D2240
Hardness, Shore D 56
56
ASTM D2240
Tensile Strength 31.0 MPa
4500 psi
ASTM D412
Elongation at Break 420 %
420 %
ASTM D412
100% Modulus 0.0120 GPa
1.74 ksi
ASTM D412
300% Modulus 0.0200 GPa
2.90 ksi
ASTM D412
Tear Strength 140 kN/m
799 pli
ASTM D624
Processing Properties Metric English Comments
Processing Temperature 190 - 210 °C
374 - 410 °F
Users viewing this material also viewed the following: