Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Processing Temperature = 1112 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1005 Wilaform Gold
Hard red gold alloy for used in decoration manufacturing.Applications: casting, chains, laminar decorationDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1023 Wilaform Gold
Hard yellow gold alloy with good extensibility. Particularly suitable for by machine manufactured decoration.Applications: casting, chains, coin/shape, laminar decorationDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1101 Wilaform Gold
Hard yellow gold alloy with good extensibility. Universally applicable in decoration manufacturing.Applications: casting, chainsDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1114 Wilaform Gold
Hard yellow gold alloy with good extensibility. Universally applicable in decoration manufacturing.Applications: casting, chains, coin/shape, laminar decoration, pipes, tubingDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1401 Wilaform Gold
Hard standard yellow gold alloy. Easily splintered and polished thus very well suited for crafts and industrial decoration manufacturing.Applications: casting, chains, laminar decoration, pipes, tu..
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1403 Wilaform Gold
Hard yellow gold alloy. Universally applicable in decoration production. Since it does not posses a very fine-grained structure it is used frequently for chainsApplications: casting, chains, lamin..
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1407 Wilaform Gold
Red gold for all kinds of decoration manufacturing.Applications: casting, chains, laminar decoration, pipes, tubingDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1408 Wilaform Gold
Hard yellow gold alloy. Easily splintered and polished.Applications: casting, laminar decoration, tubingDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1410 Wilaform Gold
Yield alloy. Particularly suitable for the production of strongly deformed or thick chains.Applications: casting, chains, coin/shapeDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1416 Wilaform Gold
Hard yellow gold alloy with good extensibility. By grain stabilization particularly suitable for the production of chains or poured parts.Applications: casting, chains, laminar decoration, pipesDen..
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1601 Wilaform Gold
Soft yellow gold alloy, ideally for the production of strongly deformed parts in decoration manufacturing and for metal coinage.Applications: casting, chains, coin/shape, laminar decoration, pipes, ..
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1602 Wilaform Gold
Hard standard yellow gold alloy. Easily splintered and polished thus very well suited for crafts and industrial decoration manufacturing.Applications: casting, chains, laminar decoration, pipes, tu..
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1604 Wilaform Gold
Rose gold for all kinds of decoration manufacturingApplications: casting, laminar decoration, pipes, tubingDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1605 Wilaform Gold
Red gold for all kinds of decoration manufacturing.Applications: casting, laminar decoration, pipes, tubingDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1608 Wilaform Gold
Universally applicable yellow gold alloy.Applications: casting, chains, laminar decoration, pipes, tubingDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1651 Wilaform Gold
High-quality alloy for all kinds of decoration production.Applications: casting, coin/shape, laminar decoration, pipes, tubingDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1701 Wilaform Gold
Yield alloy particularly suitable for coin and medal production. Also can be welded into platinum suitably.Applications: coin/shapeDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1703 Wilaform Gold
Yield alloy particularly suitable for coin and medal production.Applications: casting, chains, coin/shape, laminar decoration, tubingDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1907 Wilaform Gold
Palladium white gold alloy with beautiful grey-white color.Applications: casting, chains, laminar decoration, pipes, tubingDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1909 Wilaform Gold
Hard palladium white gold alloy with beautiful white color.Applications: casting, chains, laminar decoration, pipes, tubingDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1910 Wilaform Gold
Nickel and palladium-free white gold alloy with beautiful white color.Applications: casting, laminar decoration, pipes, tubingDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1911 Wilaform Gold
Hard palladium white gold alloy with beautiful white color.Applications: casting, chains, laminar decoration, pipes, tubingDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1914 Wilaform Gold
Nickel and palladium-free white gold alloy with beautiful white color.Applications: casting, laminar decoration, pipes, tubingDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1915 Wilaform Gold
Yield palladium white gold alloy with beautiful grey color. Well suitable for seizing stones.Applications: chains, coin/shape, laminar decoration, tubingDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1916 Wilaform Gold
Hard palladium white gold alloy with beautiful grey color.Applications: casting, chains, laminar decoration, pipes, tubingDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1964 Wilaform Gold
Fine gold. Universally applicable for sheet metals, volumes, pipes, profiles and contacts.Applications: chains, coin/shape, pipesDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 3011 Wilaform Silver
Universally applicable silver alloyApplications: casting, chains, coin/shape, laminar decoration, pipes, tubingDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 3012 Wilaform Silver
A balance of manufacturing and performance characteristics makes this the preferential silver alloy in the decoration manufacturing industry. The alloy unites good ductility properties with the nec..
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 3013 Wilaform Silver
Universally applicable silver alloy.Applications: casting, chains, coin/shape, laminar decoration, pipes, tubingDental
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Wieland 1001 Wilaform Gold
Hard 333/standard yellow gold alloy. Particularly suited for strongly stressed parts.Applications: casting, laminar decoration, pipes, tubingDental
Copyright © lookpolymers.com All Rights Reserved