Material Notes:
Nickel and palladium-free white gold alloy with beautiful white color.Applications: casting, laminar decoration, pipes, tubingDental
Physical Properties Metric English Comments
Density 13.1 g/cc
0.473 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 200
200
HV5; glowed
Tensile Strength, Ultimate 745 MPa
108000 psi
Elongation at Break 45 %
45 %
Thermal Properties Metric English Comments
Melting Point 840 - 860 °C
1540 - 1580 °F
Solidus 840 °C
1540 °F
Liquidus 860 °C
1580 °F
Component Elements Properties Metric English Comments
Cobalt, Co 0.70 %
0.70 %
Copper, Cu 20.4 %
20.4 %
Gold, Au 59 %
59 %
Manganese, Mn 8.4 %
8.4 %
Silver, Ag 11 %
11 %
Zinc, Zn 0.50 %
0.50 %
Processing Properties Metric English Comments
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Casting Temperature 960 - 1060 °C
1760 - 1940 °F
Descriptive Properties Value Comments
Color white