Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wieland 1601 Wilaform Gold

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy
Manufacturer Wieland
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland 1601 Wilaform Gold.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Soft yellow gold alloy, ideally for the production of strongly deformed parts in decoration manufacturing and for metal coinage.Applications: casting, chains, coin/shape, laminar decoration, pipes, tubingDental
Physical Properties Metric English Comments
Density 15.7 g/cc
0.567 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 90
90
HV5; glowed
Tensile Strength, Ultimate 300 MPa
43500 psi
Elongation at Break 45 %
45 %
Thermal Properties Metric English Comments
Melting Point 920 - 950 °C
1690 - 1740 °F
Solidus 920 °C
1690 °F
Liquidus 950 °C
1740 °F
Component Elements Properties Metric English Comments
Copper, Cu 6.0 %
6.0 %
Gold, Au 75 %
75 %
Silver, Ag 19 %
19 %
Processing Properties Metric English Comments
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Casting Temperature 1050 - 1150 °C
1920 - 2100 °F
Descriptive Properties Value Comments
Color yellow