Wieland 1403 Wilaform Gold

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy
Manufacturer Wieland
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland 1403 Wilaform Gold.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hard yellow gold alloy. Universally applicable in decoration production. Since it does not posses a very fine-grained structure it is used frequently for chainsApplications: casting, chains, laminar decorationDental
Physical Properties Metric English Comments
Density 14.0 g/cc
0.506 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 120
120
HV5; glowed
Tensile Strength, Ultimate 400 MPa
58000 psi
Elongation at Break 33 %
33 %
Thermal Properties Metric English Comments
Melting Point 870 - 920 °C
1600 - 1690 °F
Solidus 870 °C
1600 °F
Liquidus 920 °C
1690 °F
Component Elements Properties Metric English Comments
Copper, Cu 0.26 %
0.26 %
Gold, Au 58.5 %
58.5 %
Silver, Ag 33.5 %
33.5 %
Zinc, Zn 7.74 %
7.74 %
Processing Properties Metric English Comments
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Casting Temperature 1020 - 1120 °C
1870 - 2050 °F
Descriptive Properties Value Comments
Color pale-yellow