Wieland 3011 Wilaform Silver

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy
Manufacturer Wieland
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland 3011 Wilaform Silver.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Universally applicable silver alloyApplications: casting, chains, coin/shape, laminar decoration, pipes, tubingDental
Physical Properties Metric English Comments
Density 10.2 g/cc
0.368 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 80
80
HV5; glowed
Tensile Strength, Ultimate 320 MPa
46400 psi
Elongation at Break 25 %
25 %
Thermal Properties Metric English Comments
Melting Point 780 - 840 °C
1440 - 1540 °F
Solidus 780 °C
1440 °F
Liquidus 840 °C
1540 °F
Component Elements Properties Metric English Comments
Copper, Cu 16.5 %
16.5 %
Silver, Ag 83.5 %
83.5 %
Processing Properties Metric English Comments
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Casting Temperature 940 - 1040 °C
1720 - 1900 °F
Descriptive Properties Value Comments
Color white