Wieland 1703 Wilaform Gold

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy
Manufacturer Wieland
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland 1703 Wilaform Gold.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Yield alloy particularly suitable for coin and medal production.Applications: casting, chains, coin/shape, laminar decoration, tubingDental
Physical Properties Metric English Comments
Density 17.6 g/cc
0.636 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 70
70
HV5; glowed
Tensile Strength, Ultimate 300 MPa
43500 psi
Elongation at Break 35 %
35 %
Thermal Properties Metric English Comments
Melting Point 960 - 990 °C
1760 - 1810 °F
Solidus 960 °C
1760 °F
Liquidus 990 °C
1810 °F
Component Elements Properties Metric English Comments
Copper, Cu 4.0 %
4.0 %
Gold, Au 90 %
90 %
Silver, Ag 6.0 %
6.0 %
Processing Properties Metric English Comments
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Casting Temperature 1090 - 1190 °C
1990 - 2170 °F
Descriptive Properties Value Comments
Color full-yellow