Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wieland 1410 Wilaform Gold

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy
Manufacturer Wieland
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland 1410 Wilaform Gold.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Yield alloy. Particularly suitable for the production of strongly deformed or thick chains.Applications: casting, chains, coin/shapeDental
Physical Properties Metric English Comments
Density 14.1 g/cc
0.509 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 85
85
HV5; glowed
Tensile Strength, Ultimate 350 MPa
50800 psi
Elongation at Break 33 %
33 %
Thermal Properties Metric English Comments
Melting Point 870 - 930 °C
1600 - 1710 °F
Solidus 870 °C
1600 °F
Liquidus 930 °C
1710 °F
Component Elements Properties Metric English Comments
Copper, Cu 4.84 %
4.84 %
Gold, Au 58.5 %
58.5 %
Silver, Ag 35.5 %
35.5 %
Zinc, Zn 1.16 %
1.16 %
Processing Properties Metric English Comments
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Casting Temperature 1030 - 1130 °C
1890 - 2070 °F
Descriptive Properties Value Comments
Color green yellow 0N