Material Notes:
Hard yellow gold alloy with good extensibility. By grain stabilization particularly suitable for the production of chains or poured parts.Applications: casting, chains, laminar decoration, pipesDental
Physical Properties Metric English Comments
Density 12.9 g/cc
0.466 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 120
120
HV5; glowed
Thermal Properties Metric English Comments
Melting Point 840 - 870 °C
1540 - 1600 °F
Solidus 840 °C
1540 °F
Liquidus 870 °C
1600 °F
Component Elements Properties Metric English Comments
Copper, Cu 29.37 %
29.37 %
Gold, Au 58.5 %
58.5 %
Silver, Ag 6.0 %
6.0 %
Zinc, Zn 6.13 %
6.13 %
Processing Properties Metric English Comments
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Casting Temperature 970 - 1070 °C
1780 - 1960 °F
Descriptive Properties Value Comments
Color reddish-yellow
Users viewing this material also viewed the following: