Wieland 1911 Wilaform Gold

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy
Manufacturer Wieland
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland 1911 Wilaform Gold.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hard palladium white gold alloy with beautiful white color.Applications: casting, chains, laminar decoration, pipes, tubingDental
Physical Properties Metric English Comments
Density 15.8 g/cc
0.571 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 140
140
HV5; glowed
Thermal Properties Metric English Comments
Melting Point 1020 - 1080 °C
1870 - 1980 °F
Solidus 1020 °C
1870 °F
Liquidus 1080 °C
1980 °F
Component Elements Properties Metric English Comments
Copper, Cu 10 %
10 %
Gold, Au 75 %
75 %
Palladium, Pd 10 %
10 %
Silver, Ag 5.0 %
5.0 %
Processing Properties Metric English Comments
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Casting Temperature 1180 - 1280 °C
2160 - 2340 °F
Descriptive Properties Value Comments
Color white