Wieland 1701 Wilaform Gold

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy
Manufacturer Wieland
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland 1701 Wilaform Gold.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Yield alloy particularly suitable for coin and medal production. Also can be welded into platinum suitably.Applications: coin/shapeDental
Physical Properties Metric English Comments
Density 19.0 g/cc
0.686 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 40
40
HV5; glowed
Tensile Strength, Ultimate 200 MPa
29000 psi
Elongation at Break 35 %
35 %
Thermal Properties Metric English Comments
Melting Point 1020 - 1040 °C
1870 - 1900 °F
Solidus 1020 °C
1870 °F
Liquidus 1040 °C
1900 °F
Component Elements Properties Metric English Comments
Copper, Cu 1.4 %
1.4 %
Gold, Au 98.6 %
98.6 %
Processing Properties Metric English Comments
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Casting Temperature 1140 - 1240 °C
2080 - 2260 °F
Descriptive Properties Value Comments
Color full-yellow