Wieland 3013 Wilaform Silver

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy
Manufacturer Wieland
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland 3013 Wilaform Silver.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Universally applicable silver alloy.Applications: casting, chains, coin/shape, laminar decoration, pipes, tubingDental
Physical Properties Metric English Comments
Density 10.4 g/cc
0.376 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 70
70
HV5; glowed
Tensile Strength, Ultimate 300 MPa
43500 psi
Elongation at Break 30 %
30 %
Thermal Properties Metric English Comments
Melting Point 820 - 910 °C
1510 - 1670 °F
Solidus 820 °C
1510 °F
Liquidus 910 °C
1670 °F
Component Elements Properties Metric English Comments
Copper, Cu 6.5 %
6.5 %
Silver, Ag 93.5 %
93.5 %
Processing Properties Metric English Comments
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Casting Temperature 1010 - 1100 °C
1850 - 2010 °F
Descriptive Properties Value Comments
Color white