Polymer Property : CTE, linear = 13.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 °C
13.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ravago Manufacturing Americas Hylon® N1033HL Nylon 6/6 (DAM)
Information provided by Ravago.
CTE, linear 23.4 µm/m-°C

@Temperature -40.0 - 149 °C
13.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Duratron® PBI CU60 Polybenzimidazole, unfilled, compression molded (ASTM Product Data Sheet)
Duratron® PBI is the highest performance engineering plastic available from Quadrant EPP. It offers the highest mechanical properties of any thermoplastic above 400° F (205° C). Duratron® PBI ..
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 °C
13.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ravago Manufacturing Americas Hylon® N1033L Nylon 6/6 (DAM)  (discontinued **)
Information provided by Ravago.
CTE, linear 23.4 - 30.0 µm/m-°C
13.0 - 16.7 µin/in-°F
Average value: 26.4 µm/m-°C Grade Count:4
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%..
CTE, linear 23.4 - 101 µm/m-°C
13.0 - 56.0 µin/in-°F
Average value: 65.1 µm/m-°C Grade Count:11
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v..
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 - 100 °C
13.0 µin/in-°F

@Temperature 68.0 - 212 °F
Kaiser 7068 T6, T651 Rod & Bar
Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig..
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 - 100 °C
13.0 µin/in-°F

@Temperature 68.0 - 212 °F
Kaiser 7068 T6, T6511 Rod & Bar
Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig..
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 - 100 °C
13.0 µin/in-°F

@Temperature 68.0 - 212 °F
Kaiser 7068 T76, T76511 Rod & Bar
Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig..
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 °C
13.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Techmer ES Plaslube® J-1850/30/TF/15 PBT, 30% GFR, 15% PTFE
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 °C
13.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Techmer ES Electrafil® J-50/CF/20 Polycarbonate, 20% Carbon Fiber Reinforced
Carbon Fiber Reinforced
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 - 100 °C
13.0 µin/in-°F

@Temperature 68.0 - 212 °F
average
Alcoa Excalibar® 6013-T8 Aluminum, 0.3-1.9 cm diameter
Weldability = A; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6013 characteristics and uses: High strength and good corrosion resistance...
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 - 100 °C
13.0 µin/in-°F

@Temperature 68.0 - 212 °F
average
Alcoa Excalibar® 6013-T8 Aluminum, 1.9-3.8 cm diameter
Weldability = A; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6013 characteristics and uses: High strength and good corrosion resistance...
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 - 100 °C
13.0 µin/in-°F

@Temperature 68.0 - 212 °F
average
Alcoa Excalibar® 6013-T8 Aluminum, 3.8-8.2 cm diameter
Weldability = A; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6013 characteristics and uses: High strength and good corrosion resistance...
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 - 100 °C
13.0 µin/in-°F

@Temperature 68.0 - 212 °F
average
Alcoa Excalibar® 6013-T651 Aluminum
Alcoa recommends as a higher machinability alternative to 6061-T651. It has the potential for higher machining speeds and feed rates, easier deburring,ease of clearing 'chips' and better finishes. ..
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 - 100 °C
13.0 µin/in-°F

@Temperature 68.0 - 212 °F
Constellium DOKIMA® Rolled Plate Aluminum
DOKIMA® rolled plates have moderate strength properties, a very low level of impurities, an excellent corrosion resistance, a very good dimensional stability and high thermal and electrical conduct..
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 - 100 °C
13.0 µin/in-°F

@Temperature 68.0 - 212 °F
Constellium PLAN 6061 Aluminum Rolled Plate
Rolled plates in 6061 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6061 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv..
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 - 100 °C
13.0 µin/in-°F

@Temperature 68.0 - 212 °F
Constellium PLAN 6082 Aluminum Rolled Plate
Rolled plates in 6082 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6082 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv..
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 - 100 °C
13.0 µin/in-°F

@Temperature 68.0 - 212 °F
Constellium Planoxal® 60 Aluminum plate
The advantage of Planoxal®-60 plates over other standard EN AW-6082 alloy products is their low level of internal stress. They are also suitable for technical anodizing. Planoxal®-60 is mainly use..
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 - 100 °C
13.0 µin/in-°F

@Temperature 68.0 - 212 °F
Constellium ALPLAN® 6061 Rolled Precision Aluminum Plate, Milled Both Sides
Precision plates in ALPLAN® 6061 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta..
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 - 100 °C
13.0 µin/in-°F

@Temperature 68.0 - 212 °F
Constellium ALPLAN® 6082 Rolled Precision Aluminum Plate, Milled Both Sides
Precision plates in ALPLAN® 6082 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta..
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 °C
13.0 µin/in-°F

@Temperature 68.0 °F
ALIMEX PLANAL 6082 T651 Aluminum Alloy
Aluminium rolled plates which have been machined on both sides. Has a precise surface finish and high tensile strength. The temper values and the material conditions are not changed by surface-machi..
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 °C
13.0 µin/in-°F

@Temperature 68.0 °F
ALIMEX PLANAL 7075 T651/T652 Aluminum Alloy
Aluminium rolled plates which have been machined on both sides. Has a precise surface finish and high tensile strength. The temper values and the material conditions are not changed by surface-machi..
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 °C
13.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Kasei Thermylene® P7-40FG-0600 40% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 °C
13.0 µin/in-°F

@Temperature 68.0 °F
ALIMEX 6082 T651 Aluminum Alloy Rolled
Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress relieved by stretching a controlled amount and then artificially aged.
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 °C
13.0 µin/in-°F

@Temperature 68.0 °F
ALIMEX 7075 T651/T652 Aluminum Alloy Rolled
Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress-relieved by stretching a controlled amount then artificially aged. / Solution..
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 °C
13.0 µin/in-°F

@Temperature 68.0 °F
ALIMEX AMP 8000 Aluminum Plate
AMP 8000 offers higher strength levels, good machinability and dimensional stability. Its tensile strength is up to 40% higher than AlZn5.5MgCu (7075). Moulding, (Prototypes) injection moulds, Jig ..
CTE, linear 23.4 - 58.0 µm/m-°C
13.0 - 32.2 µin/in-°F
Average value: 36.3 µm/m-°C Grade Count:19
Overview of materials for Polycarbonate, Glass + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value..
CTE, linear 23.4 µm/m-°C
13.0 µin/in-°F
BCC Products BC 5010 Epoxy Laminating System
BC 5010 is a high quality, low viscosity room temperature curing laminating resin. A Safety System for the production of a variety of dimensionally stable fiberglass tools. BC 5010 features low odor..