Material Notes:
Aluminium rolled plates which have been machined on both sides. Has a precise surface finish and high tensile strength. The temper values and the material conditions are not changed by surface-machining and clearing away of the rolled surface on both sides.Information provided by ALIMEX GmbHSolution heat-treated, stress-relieved by stretching a controlled amount and then artificially aged. / Solution heat treated, stress relieved by compressing to produce a permanent set of 1% to 5% and then artificially aged.
Physical Properties Metric English Comments
Density 2.77 g/cc
0.100 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 105 - 160
105 - 160
Tensile Strength, Ultimate 360 - 540 MPa
52200 - 78300 psi
Rm
Tensile Strength, Yield 260 - 470 MPa

@Strain 0.200 %
37700 - 68200 psi

@Strain 0.200 %
Elongation at Break <= 6.0 %
<= 6.0 %
Modulus of Elasticity 70.0 GPa
10200 ksi
Thermal Properties Metric English Comments
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 °C
13.0 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 130.0 - 160.0 W/m-K
902.2 - 1110 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000435 - 0.00000526 ohm-cm
0.00000435 - 0.00000526 ohm-cm
Descriptive Properties Value Comments
Machinability Good
Protective Anodizing Suitable, not decorative
Welding Properties (WIG, MIG) Less Suitable