Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 59.4 - 101 µm/m-°C | 33.0 - 56.0 µin/in-°F | Average value: 88.3 µm/m-°C Grade Count:21 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max.. |
|||
CTE, linear | 38.3 - 101 µm/m-°C | 21.3 - 56.0 µin/in-°F | Average value: 79.9 µm/m-°C Grade Count:8 |
Overview of materials for PVC/Acrylic Alloy This property data is a summary of similar materials in the MatWeb database for the category "PVC/Acrylic Alloy". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
CTE, linear | 18.0 - 101 µm/m-°C | 10.0 - 56.0 µin/in-°F | Average value: 91.5 µm/m-°C Grade Count:19 |
Overview of materials for ECTFE Fluoropolymer This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
CTE, linear | 23.4 - 101 µm/m-°C | 13.0 - 56.0 µin/in-°F | Average value: 65.1 µm/m-°C Grade Count:11 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
CTE, linear | 75.6 - 101 µm/m-°C @Temperature 20.0 °C |
42.0 - 56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R20 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
CTE, linear | 75.6 - 101 µm/m-°C @Temperature 20.0 °C |
42.0 - 56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R21 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
CTE, linear | 75.6 - 101 µm/m-°C @Temperature 20.0 °C |
42.0 - 56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R24 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
CTE, linear | 75.6 - 101 µm/m-°C @Temperature 20.0 °C |
42.0 - 56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R26 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
CTE, linear | 75.6 - 101 µm/m-°C @Temperature 20.0 °C |
42.0 - 56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R52 PVC/Acrylic Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
CTE, linear | 75.6 - 101 µm/m-°C @Temperature 20.0 °C |
42.0 - 56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R84 Weather Resistant Sheet Description: Weather Resistant SheetInformation provided by Spartech. |
|||
CTE, linear | 75.6 - 101 µm/m-°C @Temperature 20.0 °C |
42.0 - 56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R84/21 Weather Resistant Sheet Description: Weather Resistant SheetInformation provided by Spartech. |
|||
CTE, linear | 75.6 - 101 µm/m-°C @Temperature 20.0 °C |
42.0 - 56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R910 PC/ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
CTE, linear | 52.2 - 101 µm/m-°C | 29.0 - 56.0 µin/in-°F | Average value: 75.7 µm/m-°C Grade Count:14 |
Overview of materials for Acrylic, Optical Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr.. |
|||
CTE, linear | 75.6 - 101 µm/m-°C @Temperature 20.0 °C |
42.0 - 56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R12 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |