Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 20.0 - 30.0 µm/m-°C @Temperature 50.0 - 100 °C |
11.1 - 16.7 µin/in-°F @Temperature 122 - 212 °F |
ISO 11359-2 |
Raschig Group AMPLA® 7250 melamine-modified polyester Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow.. |
|||
CTE, linear | 20.0 - 30.0 µm/m-°C @Temperature 50.0 - 100 °C |
11.1 - 16.7 µin/in-°F @Temperature 122 - 212 °F |
ISO 11359-2 |
Raschig Group AMPLA® 7500 melamine-modified polyester Organically and inorganically filled melamine modified Polyester molding compound. Low post-shrinkage, very good electrical values, excellent heat resistance, very good sliding behavior and wear sta.. |
|||
CTE, linear | 21.0 - 30.0 µm/m-°C | 11.7 - 16.7 µin/in-°F | Average value: 22.7 µm/m-°C Grade Count:7 |
Overview of materials for Epoxy, Molded, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Mineral Filled". Each property range of values reported is minimum and maximum values of .. |
|||
CTE, linear | 12.0 - 30.0 µm/m-°C | 6.67 - 16.7 µin/in-°F | Average value: 18.4 µm/m-°C Grade Count:14 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
CTE, linear | 23.4 - 30.0 µm/m-°C | 13.0 - 16.7 µin/in-°F | Average value: 26.4 µm/m-°C Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
CTE, linear | 9.00 - 30.0 µm/m-°C | 5.00 - 16.7 µin/in-°F | Average value: 14.1 µm/m-°C Grade Count:8 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be.. |
|||
CTE, linear | 10.0 - 30.0 µm/m-°C | 5.56 - 16.7 µin/in-°F | Average value: 19.6 µm/m-°C Grade Count:26 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
CTE, linear | 19.8 - 30.0 µm/m-°C | 11.0 - 16.7 µin/in-°F | Average value: 22.5 µm/m-°C Grade Count:5 |
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
CTE, linear | 15.0 - 30.0 µm/m-°C @Temperature 20.0 - 100 °C |
8.33 - 16.7 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMINEX® 2140 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled Application: bearing shells and bearing collarsInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 15.0 - 30.0 µm/m-°C @Temperature 20.0 - 100 °C |
8.33 - 16.7 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMINEX® 2100 Cotton Fabric, Phenolic Resin Impregnated Application: bearing shells and bearing collarsInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 25.0 - 30.0 µm/m-°C | 13.9 - 16.7 µin/in-°F | |
Master Bond EP112FLAN-1 Two Component Flexibilized Heat Curing Epoxy Master Bond EP112FLAN-1 is a toughened two component, high performance epoxy resin system featuring good temperature resistance, high thermal conductivity, fine electrical insulation values and soun.. |
|||
CTE, linear | 25.0 - 30.0 µm/m-°C | 13.9 - 16.7 µin/in-°F | |
Master Bond EP112FLAO-1 Toughened, Two component, Heat Curing Epoxy Master Bond EP112FLAO-1 is a toughened two component, high performance epoxy resin system featuring very good temperature resistance, fine thermal conductivity and electrical insulation values with .. |
|||
CTE, linear | 25.0 - 30.0 µm/m-°C | 13.9 - 16.7 µin/in-°F | |
Master Bond EP45HTQ Quartz Filled Heat Resistant Epoxy Description: Master Bond Polymer Compound EP45HTQ is a two component quartz filled, epoxy compound for high performance structural bonding and casting. It is suitable for applications where long ter.. |
|||
CTE, linear | 20.0 - 30.0 µm/m-°C @Temperature 20.0 °C |
11.1 - 16.7 µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
Zell-Metall Engineering Plastics Zellamid 250 GF 30 (PA6.6 + 30% glass fiber) Zellamid® 250 GF 30 (PA 6.6 + 30% Glassfibre, black) is the registered trademark for Zell-Metalls 30% glass fiber reinforced nylon grade 6.6. It offers increased strength, stiffness, creep res.. |
|||
CTE, linear | 25.0 - 30.0 µm/m-°C | 13.9 - 16.7 µin/in-°F | |
Master Bond EP42HT-2AO-1 Two Part, Cryogenically Serviceable Epoxy Description: Master Bond EP42HT-2AO-1 Black is a room temperature curable, two component epoxy adhesive, sealant, coating and casting material that meets NASA low outgassing specifications. It featu.. |
|||
CTE, linear | 20.0 - 30.0 µm/m-°C | 11.1 - 16.7 µin/in-°F | |
Hippe PA 66 GF 30 Nylon 66 30% Glass fiber Reinforced These polyamide components being reinforced with glass fiber up to 30% are not only highly wear-resistant, but also show high mechanical strength, stiffness and dimensional stability. They can also.. |
|||
CTE, linear | 20.0 - 30.0 µm/m-°C | 11.1 - 16.7 µin/in-°F | |
Hippe PBT GF 30 Polybutylene Terephthalate 30% Glass fiber Reinforced PBT GF is a highly versatile, semi-crystalline structural thermoplastic reinforced with 30% glass fiber, with very high rigidity and strength characteristics and excellent electrical insulation prop.. |
|||
CTE, linear | 20.0 - 30.0 µm/m-°C @Temperature 20.0 °C |
11.1 - 16.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
E-Polymers TEKAMID® TA250G45 , 45% Glass Fiber Reinforced PA66, DAM 45% Glass Fiber Reinforced, Good surfaceInformation provided by E-Polymers Co. Ltd. |
|||
CTE, linear | 10.0 - 30.0 µm/m-°C @Temperature 20.0 °C |
5.56 - 16.7 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance BCN-11 Bonded (Composite) Magnetic Material |
|||
CTE, linear | 10.0 - 30.0 µm/m-°C @Temperature 20.0 °C |
5.56 - 16.7 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance BCN-13 Bonded (Composite) Magnetic Material |
|||
CTE, linear | 20.0 - 30.0 µm/m-°C | 11.1 - 16.7 µin/in-°F | VDE 0304T1 |
Bulk Molding Compounds tetra-DUR F 4308 Bulk Molding Compound UL-licensedTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), thermal stabilit.. |
|||
CTE, linear | 10.0 - 30.0 µm/m-°C @Temperature 20.0 °C |
5.56 - 16.7 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance BCN-10 Bonded (Composite) Magnetic Material |
|||
CTE, linear | 10.0 - 30.0 µm/m-°C @Temperature 20.0 °C |
5.56 - 16.7 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance BCN-12 Bonded (Composite) Magnetic Material |
|||
CTE, linear | 10.0 - 30.0 µm/m-°C @Temperature 20.0 °C |
5.56 - 16.7 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance BCN-14 Bonded (Composite) Magnetic Material |
|||
CTE, linear | 10.0 - 30.0 µm/m-°C @Temperature 20.0 °C |
5.56 - 16.7 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance BCN-15 Bonded (Composite) Magnetic Material |
|||
CTE, linear | 10.0 - 30.0 µm/m-°C @Temperature 20.0 °C |
5.56 - 16.7 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance BCN-17 Bonded (Composite) Magnetic Material |
|||
CTE, linear | 14.0 - 30.0 µm/m-°C | 7.78 - 16.7 µin/in-°F | Average value: 20.3 µm/m-°C Grade Count:11 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
CTE, linear | 20.0 - 30.0 µm/m-°C | 11.1 - 16.7 µin/in-°F | VDE 0304T1 |
Bulk Molding Compounds tetra-DUR F 4306 Bulk Molding Compound Mechanical high grade standard productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion pr.. |