Thermal Properties Metric English Comments
CTE, linear 19.8 - 30.1 µm/m-°C

@Temperature 20.0 °C
11.0 - 16.7 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Network Polymers Kepital® F20-25
Description: Natural Acetal Copolymer, 25% Glass Reinforced GradeInformation provided by Network Polymers Inc.
CTE, linear 20.0 - 30.0 µm/m-°C

@Temperature 50.0 - 100 °C
11.1 - 16.7 µin/in-°F

@Temperature 122 - 212 °F
ISO 11359-2
Raschig Group AMPLA® 7250 melamine-modified polyester
Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow..
CTE, linear 20.0 - 30.0 µm/m-°C

@Temperature 50.0 - 100 °C
11.1 - 16.7 µin/in-°F

@Temperature 122 - 212 °F
ISO 11359-2
Raschig Group AMPLA® 7500 melamine-modified polyester
Organically and inorganically filled melamine modified Polyester molding compound. Low post-shrinkage, very good electrical values, excellent heat resistance, very good sliding behavior and wear sta..
CTE, linear 21.0 - 30.0 µm/m-°C
11.7 - 16.7 µin/in-°F
Average value: 22.7 µm/m-°C Grade Count:7
Overview of materials for Epoxy, Molded, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Mineral Filled". Each property range of values reported is minimum and maximum values of ..
CTE, linear 12.0 - 30.0 µm/m-°C
6.67 - 16.7 µin/in-°F
Average value: 18.4 µm/m-°C Grade Count:14
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum ..
CTE, linear 23.4 - 30.0 µm/m-°C
13.0 - 16.7 µin/in-°F
Average value: 26.4 µm/m-°C Grade Count:4
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%..
CTE, linear 9.00 - 30.0 µm/m-°C
5.00 - 16.7 µin/in-°F
Average value: 14.1 µm/m-°C Grade Count:8
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be..
CTE, linear 10.0 - 30.0 µm/m-°C
5.56 - 16.7 µin/in-°F
Average value: 19.6 µm/m-°C Grade Count:26
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
CTE, linear 19.8 - 30.0 µm/m-°C
11.0 - 16.7 µin/in-°F
Average value: 22.5 µm/m-°C Grade Count:5
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
CTE, linear 15.0 - 30.0 µm/m-°C

@Temperature 20.0 - 100 °C
8.33 - 16.7 µin/in-°F

@Temperature 68.0 - 212 °F
DIN 53752
Schwartz Technical Plastics LAMINEX® 2140 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled
Application: bearing shells and bearing collarsInformation provided by Schwartz Technical Plastics GmbH
CTE, linear 15.0 - 30.0 µm/m-°C

@Temperature 20.0 - 100 °C
8.33 - 16.7 µin/in-°F

@Temperature 68.0 - 212 °F
DIN 53752
Schwartz Technical Plastics LAMINEX® 2100 Cotton Fabric, Phenolic Resin Impregnated
Application: bearing shells and bearing collarsInformation provided by Schwartz Technical Plastics GmbH
CTE, linear 25.0 - 30.0 µm/m-°C
13.9 - 16.7 µin/in-°F
Master Bond EP112FLAN-1 Two Component Flexibilized Heat Curing Epoxy
Master Bond EP112FLAN-1 is a toughened two component, high performance epoxy resin system featuring good temperature resistance, high thermal conductivity, fine electrical insulation values and soun..
CTE, linear 25.0 - 30.0 µm/m-°C
13.9 - 16.7 µin/in-°F
Master Bond EP112FLAO-1 Toughened, Two component, Heat Curing Epoxy
Master Bond EP112FLAO-1 is a toughened two component, high performance epoxy resin system featuring very good temperature resistance, fine thermal conductivity and electrical insulation values with ..
CTE, linear 25.0 - 30.0 µm/m-°C
13.9 - 16.7 µin/in-°F
Master Bond EP45HTQ Quartz Filled Heat Resistant Epoxy
Description: Master Bond Polymer Compound EP45HTQ is a two component quartz filled, epoxy compound for high performance structural bonding and casting. It is suitable for applications where long ter..
CTE, linear 20.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 68.0 °F
DIN 53752
Zell-Metall Engineering Plastics Zellamid 250 GF 30 (PA6.6 + 30% glass fiber)
Zellamid® 250 GF 30 (PA 6.6 + 30% Glassfibre, black) is the registered trademark for Zell-Metall’s 30% glass fiber reinforced nylon grade 6.6. It offers increased strength, stiffness, creep res..
CTE, linear 25.0 - 30.0 µm/m-°C
13.9 - 16.7 µin/in-°F
Master Bond EP42HT-2AO-1 Two Part, Cryogenically Serviceable Epoxy
Description: Master Bond EP42HT-2AO-1 Black is a room temperature curable, two component epoxy adhesive, sealant, coating and casting material that meets NASA low outgassing specifications. It featu..
CTE, linear 20.0 - 30.0 µm/m-°C
11.1 - 16.7 µin/in-°F
Hippe PA 66 GF 30 Nylon 66 30% Glass fiber Reinforced
These polyamide components being reinforced with glass fiber up to 30% are not only highly wear-resistant, but also show high mechanical strength, stiffness and dimensional stability. They can also..
CTE, linear 20.0 - 30.0 µm/m-°C
11.1 - 16.7 µin/in-°F
Hippe PBT GF 30 Polybutylene Terephthalate 30% Glass fiber Reinforced
PBT GF is a highly versatile, semi-crystalline structural thermoplastic reinforced with 30% glass fiber, with very high rigidity and strength characteristics and excellent electrical insulation prop..
CTE, linear 20.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 68.0 °F
ASTM D696
E-Polymers TEKAMID® TA250G45 , 45% Glass Fiber Reinforced PA66, DAM
45% Glass Fiber Reinforced, Good surfaceInformation provided by E-Polymers Co. Ltd.
CTE, linear 10.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
5.56 - 16.7 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance BCN-11 Bonded (Composite) Magnetic Material
CTE, linear 10.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
5.56 - 16.7 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance BCN-13 Bonded (Composite) Magnetic Material
CTE, linear 20.0 - 30.0 µm/m-°C
11.1 - 16.7 µin/in-°F
VDE 0304T1
Bulk Molding Compounds tetra-DUR F 4308 Bulk Molding Compound
UL-licensedTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), thermal stabilit..
CTE, linear 10.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
5.56 - 16.7 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance BCN-10 Bonded (Composite) Magnetic Material
CTE, linear 10.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
5.56 - 16.7 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance BCN-12 Bonded (Composite) Magnetic Material
CTE, linear 10.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
5.56 - 16.7 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance BCN-14 Bonded (Composite) Magnetic Material
CTE, linear 10.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
5.56 - 16.7 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance BCN-15 Bonded (Composite) Magnetic Material
CTE, linear 10.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
5.56 - 16.7 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance BCN-17 Bonded (Composite) Magnetic Material
CTE, linear 14.0 - 30.0 µm/m-°C
7.78 - 16.7 µin/in-°F
Average value: 20.3 µm/m-°C Grade Count:11
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..
CTE, linear 20.0 - 30.0 µm/m-°C
11.1 - 16.7 µin/in-°F
VDE 0304T1
Bulk Molding Compounds tetra-DUR F 4306 Bulk Molding Compound
Mechanical high grade standard productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion pr..